Intraoral repairs often involve bonding composite to fractured porcelain. Newer adhesive systems, currently referred to as multipurpose systems, include materials with recommended procedures for repair of porcelain. This laboratory study evaluated various treatment regimens with the ProBond adhesive system. Three different porcelain surface procedures were used: (1) air abrasion with aluminum oxide (50 microm), (2) 8% hydrofluoric acid, and (3) air abrasion and hydrofluoric acid. Eight different treatment procedures were then used to bond 10 composite cylinders to porcelain surfaces in each group. Shear bond strengths (in megapascals) were determined with an Instron testing machine after storage in water for 24 hours at 37 degrees C and after 3 months of storage and thermocycling. The combination of air abrasion and hydrofluoric acid on porcelain surfaces before bonding composite recorded the most consistently effective bond strengths. Four of the treatment regimens in the air abrasion groups yielded low bond strengths at 3 months. This study also indicated that silane treatment of porcelain is critical for development of suitable bond strengths for composite.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1016/s0022-3913(96)90294-2 | DOI Listing |
Materials (Basel)
January 2025
Division of Biomaterials, School of Dentistry, University of Alabama at Birmingham, Birmingham, AL 35209, USA.
Two 3D-printed crown materials (Crown and Ceramic Crown) were examined to determine the best surface treatment and primers for bonding. Discs of the two materials were printed and mounted with their "intaglio" surfaces untouched. Half the specimens from each group were sandblasted with 50 µm alumina.
View Article and Find Full Text PDFDent J (Basel)
December 2024
Prosthetic Dentistry Discipline, Department 4-Prosthodontics and Dental Materials, Faculty of Dental Medicine, "Iuliu Hațieganu" University of Medicine and Pharmacy, 400012 Cluj-Napoca, Romania.
Air particle abrasion (APA) is a common surface preparation method in dentistry, particularly for improving bond strength to dentin. This review evaluates the influence of APA on dentin adhesion. : A systematic literature search from 2018 to 2023 was conducted according to PRISMA-ScR guidelines.
View Article and Find Full Text PDFJ Dent
January 2025
State Key Laboratory of Oral & Maxillofacial Reconstruction and Regeneration, Key Laboratory of Oral Biomedicine Ministry of Education, Hubei Key Laboratory of Stomatology, School & Hospital of Stomatology, Wuhan University, Wuhan 430079, PR China. Electronic address:
Objectives: Highly translucent yttria-stabilized zirconia (YSZ) has become more popular due to its enhanced aesthetics. This study aimed to evaluate the influence of traditional air abrasion and a new etching and cleaning agent, Multi Etchant, on the mechanical performance, optical properties, and bond strength of highly translucent zirconia.
Methods: Specimens of 6YSZ, 5YSZ, 4YSZ&5YSZ, and conventional 3YSZ were fabricated and underwent different surface treatments, including as milled, air abrasion, and Multi Etchant.
J Dent
January 2025
Department of Dentistry, Federal University of Rio Grande do Norte, Natal, RN, Brazil. Electronic address:
Objective: To evaluate the influence of different cleaning methods, surface treatments, and aging on the repair bond strength to a CAD/CAM glass-ceramic.
Materials And Methods: Forty-eight lithium disilicate CAD/CAM ceramic blocks were fabricated, sintered, and embedded in acrylic resin. After contamination with human saliva, they were divided according to the factors "Cleaning method" (Control-water/air spray, Air-particle abrasion with AlO, Ivoclean cleaning paste), "Surface treatment" (5 % Hydrofluoric acid-HF + Silane, Monobond Etch & Prime-MEP), and "Aging" (thermocycling, no thermocycling).
J Prosthodont Res
January 2025
Institute of Dentistry, Department of Biomaterials Science and Turku Clinical Biomaterials Centre - TCBC, Turku, Finland.
Purpose: This study investigated the bond strength between short fiber-reinforced resin composite (SFC) and dentin following air abrasion with various types of abrasive particles.
Methods: A total of 120 human molars were prepared for a shear bond strength (SBS) test of the resin composite. The teeth were divided into 12 groups (n = 10/group) based on the air abrasion particle used.