Ultrathin nanocapacitor assembled via atomic layer deposition.

Nanotechnology

Universidad Nacional Autónoma de México Centro de Nanociencias y Nanotecnología, Km 107 Carretera Tijuana-Ensenada, Ensenada, B.C., C.P. 22800, Mexico, Ensenada, Baja California, 22800, MEXICO.

Published: September 2024

We fabricated ultrathin metal - oxide - semiconductor (MOS) nanocapacitors using atomic layer deposition. The capacitors consist of a bilayer of Al2O3 and Y2O3 with a total thickness of ~10 nm, deposited on silicon substrate. The presence of the two materials, each slab being ~5 nm thick and uniform over a large area, was confirmed with Transmission Electron Microscopy and X-ray photoelectron spectroscopy (XPS). The capacitance in accumulation varied from 1.6 nF (at 1MHz) to ~2.8 nF (at 10 kHz), which is one to two orders of magnitude higher than other nanocapacitors. This high capacitance is attributed to the synergy between the dielectric properties of ultrathin Al2O3 and Y2O3 layers. The electrical properties of the nanocapacitor are stable within a wide range of temperatures, from 25 °C to 150 °C, as indicated by capacitance-voltage (C - V). Since the thickness-to-area ratio is negligible, the nanocapacitor could be simulated as a single parallel plate capacitor in COMSOL Multiphysics, with good agreement between experimental and simulation data. As a proof-of-concept we simulated a MOSFET device with the nanocapacitor gate dielectric, whose drain current is sufficiently high for micro and nanoelectronics integrated circuits, including for applications in sensing.

Download full-text PDF

Source
http://dx.doi.org/10.1088/1361-6528/ad7f5cDOI Listing

Publication Analysis

Top Keywords

atomic layer
8
layer deposition
8
al2o3 y2o3
8
ultrathin nanocapacitor
4
nanocapacitor assembled
4
assembled atomic
4
deposition fabricated
4
fabricated ultrathin
4
ultrathin metal
4
metal oxide
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!