The corrosion behavior of borosilicate glass in the presence of cementitious waste forms.

Dalton Trans

Pacific Northwest National Laboratory, 902 Battelle Blvd, Richland, WA 99354, USA.

Published: July 2024

AI Article Synopsis

Article Abstract

Borosilicate glasses are widely used for radioactive waste disposal due to their ability to incorporate a variety of contaminants and radionuclides while exhibiting high durability in various disposal scenarios. This research evaluated the dissolution of borosilicate glass using both single-pass-flow-through (ASTM C1662-18) and product consistency test (ASTM C1285-21) methods with different solutions, including a cementitious-contacted water (called grout-contacted, GC, from this point) and solutions with varying levels of dissolved cementitious species such as Si, Ca, Al. The results indicated that the presence of Ca plays a crucial role in suppressing glass corrosion, as evidenced by the slower normalized dissolution rates, which were one order of magnitude lower for boron and two orders of magnitude lower for rhenium, observed in both Ca-amended and GC solutions compared to the pH 12 buffer solution. This effect is attributed to the formation of a dense, low-porosity, and strongly bonded calcium silicate hydrate (CSH) layer on the glass surface, which implies that a glass corrosion process is influenced by ion exchange involving alkali ions Na, K, Ca, and hydrogen-containing species. A small number of glass particles treated in the GC solution showed minor corrosion pits in the form of shallow craters with an average diameter of approximately 500 μm. This observation is correlated with a significant reduction, 2000 to 3000 times lower, in the cumulative volume of glass pores, indicating that smaller pore voids were "sealed" in the presence of Ca ions, likely attributed to the formation of CSH precipitation or other corrosion products such as calcium carbonate saturated from the grout solution. These findings suggest that the presence of dissolved Ca in the GC solution can slow down the dissolution of borosilicate glass, contrary to the expected trend of higher dissolution rates resulting from exposure to high alkaline and thus higher pH solutions.

Download full-text PDF

Source
http://dx.doi.org/10.1039/d4dt00855cDOI Listing

Publication Analysis

Top Keywords

borosilicate glass
12
glass
8
dissolution borosilicate
8
glass corrosion
8
dissolution rates
8
magnitude lower
8
attributed formation
8
corrosion
5
corrosion behavior
4
borosilicate
4

Similar Publications

We develop fs laser-fabricated asymmetric couplers and zig-zag arrays consisting of single- and two-mode waveguides with bipartite Kerr nonlinearity in borosilicate (BK7) glass substrates. The fundamental mode ( orbital) is near resonance with the neighboring higher-order orbital, causing efficient light transfer at low power. Due to Kerr nonlinearity, the coupler works as an all-optical switch between and orbitals.

View Article and Find Full Text PDF

Interfacial mechanisms of enhanced photoluminescence in AgI-doped red light emitting perovskite quantum dot glass.

J Colloid Interface Sci

January 2025

Institute of Optoelectronic Materials and Devices, College of Optical and Electronic Technology, China Jiliang University, Hangzhou 310018 PR China. Electronic address:

Red light emitting perovskite quantum dot (PQD) glass, with narrow-band emission and excellent stability, holds great potential for applications in liquid crystal displays. However, its low photoluminescence quantum yield (PLQY) remains the biggest obstacle limiting its practical application. Additionally, the mechanism behind the enhancement of the PLQY is not well understood, which restricts the further improvement of the PLQY in red light emitting PQD glass.

View Article and Find Full Text PDF

Rationale: Carbonate minerals are one of the most popular samples for an automated sample preparation system for CF-IRMS, such as GasBench II and iso FLOW, but no standardized analytical protocols exist. This study gives guidelines on optimal analytic conditions for carbon and oxygen isotope analysis of Ca-Mg carbonates when using the carbonate-phosphoric acid reaction method.

Methods: Calcite (CaCO-McMaster Carrara), dolomite (CaMg(CO)-MRSI Dolomite), and magnesite (MgCO-ROM Brazil Magnesite) with two grain size fractions (< 74 and 149-250 μm) were reacted with 103% (specific gravity of 1.

View Article and Find Full Text PDF

Dy and Eu co-doped borosilicate glasses have been synthesised via melt quench technique. Amorphous behaviour of the sample has been verified by XRD study. FT-IR analysis confirmed the presence of various bonds in the host lattice.

View Article and Find Full Text PDF

Bone defects resulting from trauma or diseases that lead to bone loss have created a growing need for innovative materials suitable for treating bone-related conditions. The purpose of this study is, therefore, to synthesize and analyse the synergistic effects of cerium (Ce) and cerium-silver (Ce-Ag) doping of borosilicate bioactive glass (BBG) on the bioactivity, antibacterial properties, and biocompatibility for potential applications in bone tissue engineering. This study utilized a sol-gel Stöber method to synthesize doped BBGs based on S49B4.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!