Objective: To determine the effects of conventional cigarette smoking (CS) and recent heated tobacco products (HTPs) on the surface roughness and color stability of different indirect restorative materials.

Materials And Methods: One hundred disc-shaped samples were constructed of three different restorative CAD/CAM materials: lithium disilicate glass-ceramic (IPS e.max CAD; Ivoclar Vivadent, Liechtenstein), zirconia (BruxZir® Zirconia, Glidewell, USA) and polyetheretherketone (BioHPP® bredent GmbH, Germany). Of the IPS e.max CAD and the Bruxzir samples, 20 samples were glazed, and 20 samples were polished, while the BioHPP samples were all polished according to the manufacturer's instructions. Fifty samples were subjected to conventional cigarette smoking (LM, Philip Morris International Inc., Egypt) (Groups: IPS e.max CAD_Glazed exposed to CS (LD_G_Cig), IPS e.max CAD_Polished exposed to CS (LD_P_Cig), Bruxzir_Glazed exposed to CS (Zr_G_Cig), Bruxzir _Polished exposed to CS (Zr_P_Cig) and BioHPP exposed to CS (PEEK_Cig) and fifty samples were exposed to heated tobacco product smoking (Heets, Russet selection, Philip Morris International Inc., Italy) (Groups: IPS e.max CAD_Glazed exposed to HTP (LD_G_HTP), IPS e.max CAD_Polished exposed to HTP (LD_P_HTP), Bruxzir_Glazed exposed to HTP (Zr_G_HTP), Bruxzir CAD_Polished exposed to HTP (Zr_P_HTP) and BioHPP exposed to HTP (PEEK_HTP).. Six hundred cigarettes/heets representing 30 days of medium smoking behavior (20 cigarettes/day) were used. Before and after exposure to smoke, the surface roughness of all the samples was measured using JITAI8101 surface roughness tester (Beijing Jitai Tech Detection Device Co., Ltd, China, and the color parameters were assessed using VITA Easyshade Advance 4.01 (VITA shade, VITA made, VITA). The data were analyzed using One-way ANOVA, paired sample t-test and independent sample t-test. The significance level was set at α < 0.05. The surface topography was evaluated by scanning electron microscopy (SEM) and analyzed using energy-dispersive X-ray (EDX) spectroscopy to determine changes in the surface chemical composition.

Results: Both types of smoking caused significant increases in the surface roughness of all the samples. There was a significant difference in color change between CS and HTP for all materials with different surface finish (P < 0.01) and zirconia had the greatest effect on color change (P < 0.001). In contrast, polyetheretherketone (PEEK) "BioHPP" had the least effect (P < 0.001).

Conclusion: Exposure to different types of smoking induce changes in the surface topography and color of different esthetic restorative materials. Compared with HTP, conventional cigarette smoke has a greater effect on the surface roughness and color stability of esthetic restorative materials. The glazed surfaces showed less change in surface topography than did the polished surfaces. Zirconia showed better color stability when compared to polyetheretherketone (PEEK).

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC11227156PMC
http://dx.doi.org/10.1186/s12903-024-04423-2DOI Listing

Publication Analysis

Top Keywords

ips emax
24
exposed htp
20
conventional cigarette
12
cigarette smoking
12
heated tobacco
12
surface roughness
12
cad_polished exposed
12
exposed
11
smoking heated
8
tobacco products
8

Similar Publications

Properties of New Partially Crystallized Lithium Disilicate CAD-CAM Materials.

Oper Dent

January 2025

*Kraig S. Vandewalle, DDS, MS, Col (ret), USAF, DC, Air Force Consultant in Dental Research Advanced Education in General Dentistry Residency, AF Postgraduate Dental School, Joint Base San Antonio - Lackland, TX, USA; Uniformed Services University of the Health Sciences, Bethesda, MD, USA.

Objective: The purpose of this study was to compare the optical, mechanical, and biological properties of two new, inexpensive lithium disilicate (LS2) materials (Lodden (LOD), LD Medical Technology; and BeautyZir (BZ), BeautyZir Technology) to a clinically established LS2 material (IPS e.max CAD (EMAX), Ivoclar Vivadent).

Methods And Materials: The optical properties of the translucency parameter (TP) and opalescence parameter (OP) were obtained with a dental spectrophotometer.

View Article and Find Full Text PDF

Repair Bond Strength of Composite Resin to Dental Ceramic Using Various Surface Treatments: An Study.

J Int Soc Prev Community Dent

October 2024

Department of Conservative Dentistry, College of Dentistry, University of Mosul, Mosul, Iraq.

Aim: This research aims to evaluate and compare the effect of various surface treatments and adhesive types on the bond strength between composite resin and two types of ceramic materials.

Materials And Methods: A total of 98 disk-shaped of 10 mm diameter and 4 mm thickness were fabricated for each of the zirconia (H. C.

View Article and Find Full Text PDF

Effect of thermomechanical aging on marginal fit of three CAD-CAM restorative materials: An in vitro study.

J Dent Res Dent Clin Dent Prospects

September 2024

Crown and Bridge Department, Faculty of Dental Medicine, Al Azhar University, Assiut, Egypt.

Background: The present study assessed the impact of thermomechanical aging on the marginal fit of hybrid ceramic, reinforced composite resin, and lithium disilicate ceramic.

Methods: Eighteen human upper first premolars freshly extracted for orthodontic purposes were used to fabricate 18 CAD-CAM veneers and divided into three groups based on materials used: group H (n=6): hybrid ceramics (Vita Enamic), group R (n=6): reinforced composite resin (Brilliant crios), and group L (n=6): lithium disilicate ceramic (IPS e-max CAD). Each material's cementation procedure was carried out according to the manufacturer's instructions.

View Article and Find Full Text PDF

Objectives: To compare the interfacial fracture toughness (IFT) with or without aging, of four different classes of CAD-CAM ceramic and composite materials bonded with self-adhesive resin cement to titanium alloy characteristic of implant abutments.

Methods: High translucent zirconia (Katana; KAT), lithium disilicate-based glass-ceramic (IPS. emax.

View Article and Find Full Text PDF
Article Synopsis
  • The study aimed to assess how polishing and bleaching affect the brightness, color, whiteness, and translucency of different CAD/CAM dental materials after they were stained with coffee.
  • Various treatments were applied to disks made from specific materials, with measurements taken before and after coffee exposure, and the results were analyzed statistically.
  • Ultimately, the findings indicated that the effectiveness of these treatments in restoring desired properties varies based on the specific material used.
View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!