  • The study focuses on designing fracture internal fixation implants made from biodegradable materials that have a stiffness that changes over time, to better support bone healing at different stages.
  • A mathematical model was created to simulate the degradation and mechanical behavior of composite materials, allowing for a design method that creates implants with variable density and time-varying stiffness.
  • An example involving a bone plate for tibial fractures demonstrated that the biodegradable plates performed better in terms of bone remodeling compared to traditional titanium and stainless steel plates, showing higher average elastic modulus after 11 months.

Article Abstract

The stiffness of an ideal fracture internal fixation implant should have a time-varying performance, so that the fracture can generate reasonable mechanical stimulation at different healing stages, and biodegradable materials meet this performance. A topology optimization design method for composite structures of fracture internal fixation implants with time-varying stiffness is proposed, considering the time-dependent degradation process of materials. Using relative density and degradation residual rate to describe the distribution and degradation state of two materials with different degradation rates and elastic modulus, a coupled mathematical model of degradation simulation mechanical analysis was established. Biomaterial composite structures were designed based on variable density method to exhibit time-varying stiffness characteristics. Taking the bone plate used for the treatment of tibial fractures as an example, a composite structure bone plate with time-varying stiffness characteristics was designed using the proposed method. The optimization results showed that material 1 with high stiffness formed a columnar support structure, while material 2 with low stiffness was distributed at the degradation boundary and inside. Using a bone remodeling simulation model, the optimized bone plates were evaluated. After 11 months of remodeling, the average elastic modulus of callus using degradable time-varying stiffness plates, titanium alloy plates, and stainless steel plates were 8 634 MPa, 8 521 MPa, and 8 412 MPa, respectively, indicating that the use of degradable time-varying stiffness plates would result in better remodeling effects on the callus.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC11208653PMC
http://dx.doi.org/10.7507/1001-5515.202311037DOI Listing

Publication Analysis

Top Keywords

time-varying stiffness
20
fracture internal
12
internal fixation
12
bone remodeling
8
fixation implants
8
implants time-varying
8
stiffness
8
composite structures
8
elastic modulus
8
stiffness characteristics
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!