Objective: This study aimed to compare the micro-shear bond strength (μSBS) of caries-affected dentin (CAD) and sound dentin (SoD) in primary and permanent teeth using an alternative self-etch application of "no wait" universal adhesive.
Methods And Materials: Flat midcoronal dentin surfaces from 72 permanent third molars and 72 second primary molars were distributed randomly into 12 groups according to the substrate SoD and artificially-created CAD (pH cycling for 14 days) and the adhesive system (GLUMA Bond5, a two-step etch & rinse adhesive, GLUMA Bond, a one-step self-etch adhesive, and Tokuyama Universal Bond, a one-step self-etch adhesive) (n=12). Bonded dentin resin discs were put through micro-shear bond strength testing after 10,000 thermocycles. The results were evaluated using two-way ANOVA and the Bonferroni test with a significance level of α = 0.05.
Results: When compared to SoD, the etch & rinse system's test results on artificially created CAD showed a statistically significant poorer bonding performance in both permanent and primary teeth in all groups (p<0.05). While the bond strengths of permanent teeth using total-etch adhesive on sound dentin were statistically significantly higher than those using Tokuyama Universal Bond adhesive (p<0.05), there was no significant difference in sound dentin in primary teeth (p>0.05).
Conclusions: The etch & rinse system performed the poorest of all adhesive systems on CAD. The Tokuyama Universal Bond's adhesive strength was similar in SoD and CAD on primary teeth. The use of Tokuyama Universal Adhesives can speed up restorative treatment in pediatric dentistry.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.2341/23-065-L | DOI Listing |
BMC Oral Health
January 2025
Department of Cariology and Operative Dentistry, Graduate School of Medical and Dental Sciences, Institute of Science Tokyo, 1-5-45 Yushima, Bunkyo-Ku, Tokyo, 113-8549, Japan.
Background: Resin cements often require substrate-specific pretreatment. Recently, universal adhesive systems have been introduced, simplifying procedures by eliminating the need for multiple adhesives and offering options that do not require light curing. This study investigated the bonding performance of universal adhesive systems combined with dual-polymerising resin cements on enamel, dentin, zirconia, lithium disilicate ceramics (LDS), and resin blocks.
View Article and Find Full Text PDFJ Dent (Shiraz)
December 2024
Dept. of Restorative Dentistry, Dental Research Center, School of Dentistry, Birjand University of Medical Sciences, Birjand, Iran.
Statement Of The Problem: One of the most important factors in the clinical longevity of composite resin restorations is proper adhesion, which is achieved using phosphoric acid. Different phosphoric acid products might affect the micro-shear bond strength of composite resin to enamel.
Purpose: The present study aimed to evaluate the micro-shear bond strength of composite resin to sound enamel using six different brands of acid-etch agents.
BDJ Open
December 2024
Department of Restorative Dental Science, College of Dentistry, Taibah University, Madinah, Saudi Arabia.
Objective: Evaluating immediate and delayed micro shear bond strength (µSBS) between composite resin and glass ionomer cements using different adhesive systems and mechanical surface treatment.
Materials And Methods: A total of 240 specimens of glass ionomer restorative materials were divided into two groups: Resin Modified Glass Ionomer Cement (RMGIC) namely Riva Light Cure and Conventional Glass Ionomer Cement (CGIC) namely Riva Self Cure. These were subdivided into immediate (24 h) and delayed (3 months) storage and further divided into smooth, medium, and rough surface treatment with either total etch (TE) or self-etch (SE) adhesive strategies.
J Int Soc Prev Community Dent
October 2024
Department of Basic Dental Science, College of Dentistry, University of Mosul, Mosul, Iraq.
Aim: To evaluate the micro-shear bond strength (µ-SBS) of resin-modified glass ionomer cement and to assess the chemical and topographical changes in the zirconia fitting surface induced by acidulated phosphate fluoride (APF) gel using scanning electron microscope (SEM) analysis and Fourier transform infrared (FTIR) spectroscopy.
Materials And Methods: Thirty-two samples were prepared from two zirconia materials, UPCERA HT White and BruxZir Solid Zirconia, milled by a computer-aided design/computer-aided manufacturing system. From each zirconia sample, six plates were prepared for FTIR and SEM testing.
Materials (Basel)
October 2024
Dentistry Graduate Program, University of Costa Rica-UCR, San José 11502, Costa Rica.
The aim of this investigation was to evaluate the effect of etching protocols on bond strength, surface roughness, and mechanical properties of a zirconia-reinforced lithium silicate (ZLS) CAD/CAM-ceramic. In total, 100 bars (ISO 6872), 75 plaques, and 25 cubes were cut from ZLS blocks(Vita Suprinity). The surfaces were standardized, crystallized and divided into five groups: 1.
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!