Aqueous zinc-ion batteries (AZIBs) are attracting worldwide attention due to their multiple merits such as extreme safety, low cost, feasible assembly, and environmentally friendly enabled by water-based electrolytes. At present, AZIBs have experienced systematic advances in battery components including cathode, anode, and electrolyte, whereas research involving separators is insufficient. The separator is the crucial component of AZIBs through providing ion transport, forming contact with electrodes, serving as a container for electrolyte, and ensuring the efficient battery operation. Considering this great yet ignored significance, it is timely to present the latest advances in design strategies, the systematic classification and summary of separators. We summarize the separator optimization strategies mainly along two approaches including the modification of the frequently used glass fiber and the exploitation of new separators. The advantages and disadvantages of the two strategies are analyzed from the material types and the characteristics of different strategies. The effects and mechanisms of various materials on regulating the uniform migration and deposition of Zn, balancing the excessively concentrated nucleation points, inhibiting the growth of dendrites, and the occurrence of side reactions were discussed using confinement, electric field regulation, ion interaction force, desolvation, etc. Finally, potential directions for further improvement and development of AZIBs separators are proposed, aiming at providing helpful guidance for this booming field.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1016/j.scib.2024.01.011 | DOI Listing |
Sci Bull (Beijing)
December 2024
School of Metallurgy and Environment, Central South University, Changsha 410083, China; Engineering Research Center of the Ministry of Education for Advanced Battery Materials, Central South University, Changsha 410083, China; National Energy Metal Resources and New Materials Key Laboratory, Central South University, Changsha 410083, China. Electronic address:
The dendrite and corrosion issues still remain for zinc anodes. Interface modification of anodes has been widely used for stabilizing zinc anodes. However, it is still quite challenging for such modification to simultaneously suppress zinc dendrites and corrosion issues.
View Article and Find Full Text PDFJ Colloid Interface Sci
December 2024
Zhejiang Provincial Engineering Research Center of Oxide Semiconductors for Environmental and Optoelectronic Applications, Institute of Wenzhou, Zhejiang University, Wenzhou 325006, PR China; State Key Laboratory of Silicon and Advanced Semiconductor Materials, School of Materials Science and Engineering, Zhejiang University, Hangzhou 310027, PR China. Electronic address:
Due to their high energy density, low cost, and environmental friendliness, aqueous zinc-ion batteries are considered a potential alternative to Li-ion batteries. However, dendrite growth and parasitic reactions of water molecules limit their practical applications. Herein, an ionic liquid additive, 1-butyl-3-methylimidazolium Bis(fluorosulfonyl)imide (BMImFSI), is introduced to regulate the electrical double layer (EDL).
View Article and Find Full Text PDFACS Appl Mater Interfaces
December 2024
Frontiers Science Center for Flexible Electronics, Xi'an Institute of Flexible Electronics, Northwestern Polytechnical University, 127 West Youyi Road, Xi'an 710072, China.
The irreversible chemistry of the Zn anode, attributed to parasitic reactions and the growth of zinc dendrites, is the bottleneck in the commercialization of aqueous zinc-ion batteries. Herein, an efficient strategy via constructing an organic protective layer configured with a honeycomb-like globular-covalent organic framework (G-COF) was constructed to enhance the interfacial stability of Zn anodes. Theoretical analyses disclose that the methoxy and imine groups in G-COF have more negative adsorption energy and electrostatic potential distribution, favorable Zn adsorption, and diffusion.
View Article and Find Full Text PDFSmall Methods
December 2024
College of Chemistry and Chemical Engineering, Chongqing University, Chongqing, 401331, P. R. China.
Aqueous zinc-ion batteries (AZIBs) are considered a promising choice for energy storage devices owing to the excellent safety and favorable capacity of the Zn anode. However, the uncontrolled dendrite growth of Zn anode severely constrains the practical applications of AZIBs. Herein, a novel ion enrichment layer of CuS is designed and constructed on the Zn foil surface to achieve dendrite-free Zn anode.
View Article and Find Full Text PDFRSC Adv
December 2024
Guangdong-Hong Kong-Macao Joint Laboratory for Intelligent Micro-Nano Optoelectronic Technology, School of Physics and Optoelectronic Engineering, School of Environmental and Chemical Engineering, Foshan University Foshan 528000 China
Aqueous zinc-ion batteries are highly praised for their cost-effectiveness, environmental friendliness, and high safety, making them an ideal choice for next-generation energy storage systems. However, the practical application of Zn metal anodes is constrained by well-known challenges such as dendrite growth and significant interfacial side reactions. This study introduces a trace amount of taurine (TAU) as a leveling additive into the electrolyte to optimize the microstructure of the electrolyte and the anode interface chemistry.
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!