Aim: The purpose of the current study was to evaluate the impact of three different denture cleansers on the strength and surface roughness of heat-polymerizing resin.
Materials And Methods: A total of 120 resin discs (10 mm in diameter and 2 mm thick) were created using a stainless steel mold for surface roughness testing and flexural strength testing (in accordance with the American Dental Association (ADA) Specification No.12). Samples were divided into one of three groups (40 samples in each group): group I: Clanden, group II: Clinsodent, group III: Fittydent. Samples were immersed in denture-cleansing solutions for 30 minutes every day, and this process was repeated over a period of 15 days. Samples were stored in distilled water at room temperature in between the immersions. A surface analyzer was utilized to compare the surface roughness of each sample before and after immersion treatments. For recording flexural strength, each sample was subjected to three-point bending test by mounting samples on Universal testing machine. Comparing mean values between groups using one-way ANOVA and the Tukeys honest significant difference (HSD) test. A significance level of 0.05 was used for all statistical calculations Results: After 15 days, the maximum change of mean surface roughness of heat-polymerizing resin was found in Clanden denture cleanser group (2.64 ± 0.12) followed by Clinsodent group (2.26 ± 0.09) and Fittydent group (1.92 ± 0.06). After 15 days, the maximum change of mean flexural strength changes of heat-polymerizing resin was found in Clanden denture cleanser group (94.78 ± 0.14), followed by Fittydent group (98.64 ± 0.03) and Clinsodent group (99.26 ± 0.21).
Conclusion: Within the limitation, the current study concluded that changes were observed in surface roughness and flexural strength of all heat-polymerizing resin samples after immersion in all three denture cleansers; but least surface roughness and flexural strength changes were observed with the Fittydent cleanser group and Clinsodent group, respectively.
Clinical Significance: Cleaning dentures is crucial for maintaining both the prosthesis and oral health; therefore, it is necessary to select a cleanser that is effective without negatively affecting the base resin's qualities over time.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.5005/jp-journals-10024-3508 | DOI Listing |
Anal Chem
December 2024
Department of Chemistry, Institutes of Biomedical Sciences, Zhongshan Hospital, Fudan University, Shanghai 200433, China.
With the aging global population, the incidence of osteoporosis (OP) is increasing, putting more individuals at risk. Since postmenopausal osteoporosis (PMOP) often remains asymptomatic until a fracture occurs, making the early clinical diagnosis of PMOP particularly challenging. In this work, the AuNPs-anchored hierarchical porous ZrO microspheres (Au/HPZOMs) is designed to assist laser desorption/ionization mass spectrometry (LDI-MS) for the requirement of serum metabolic fingerprints of PMOP, postmenopausal osteopenia (PMON), and healthy controls (HC) and realize the early diagnosis and surveillance of PMOP.
View Article and Find Full Text PDFChem Rev
December 2024
Department of Chemistry, Shanghai Key Laboratory of Molecular Catalysis and Innovative Materials, and State Key Laboratory of Molecular Engineering of Polymers, iChEM, Fudan University, Shanghai 200433, P. R. China.
Core-shell magnetic particles consisting of magnetic core and functional shells have aroused widespread attention in multidisciplinary fields spanning chemistry, materials science, physics, biomedicine, and bioengineering due to their distinctive magnetic properties, tunable interface features, and elaborately designed compositions. In recent decades, various surface engineering strategies have been developed to endow them desired properties (e.g.
View Article and Find Full Text PDFMembranes (Basel)
December 2024
Unit of Chemical Technologies, Technology Centre of Catalonia, Eurecat, 43007 Tarragona, Spain.
The urgent need for sustainable, low-emission energy solutions has positioned proton exchange membrane fuel cells (PEMFCs) as a promising technology in clean energy conversion. Polysulfone (PSF) membranes with incorporated ionic liquid (IL) and hydrophobic polydimethylsiloxane-functionalized silica (SiO-PDMS) were developed and characterized for their potential application in PEMFCs. Using a phase inversion method, membranes with various combinations of PSFs, SiO-PDMS, and 1-butyl-3-methylimidazolium triflate (BMI.
View Article and Find Full Text PDFNanomaterials (Basel)
December 2024
Guangdong Provincial Key Laboratory of Electronic Functional Materials and Devices, Huizhou University, Huizhou 516007, China.
W-doped ZnO (WZO) films were deposited on glass substrates by using RF magnetron sputtering at different substrate bias voltages, and the relationships between microstructure and optical and electrical properties were investigated. The results revealed that the deposition rate of WZO films first decreased from 8.8 to 7.
View Article and Find Full Text PDFJ Funct Biomater
December 2024
Department of Maxillofacial Orthopaedics and Orthodontics, Pomeranian Medical University in Szczecin, Al. Powst. Wlkp. 72, 70111 Szczecin, Poland.
Bacterial infections are a common cause of clinical complications associated with the use of orthodontic microimplants. Biofilm formation on their surfaces and subsequent infection of peri-implant tissues can result in either exfoliation or surgical removal of these medical devices. In order to improve the properties of microimplants, hybrid coatings enriched with silver nanoparticles, calcium, and phosphorus were investigated.
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!