Despite the huge and efficient functionalities of reduced graphene oxide (RGO) for bioengineering applications, the use of harsh chemicals and unfavorable techniques in their production remains a major challenge. Microbial production of reduced graphene oxide (RGO) using specific bacterial strains has gained interest as a sustainable and efficient method. The reduction of GO to RGO by selected bacterial strains was achieved through their enzymatic activities and resulted in the removal of oxygen functional groups from GO, leading to the formation of RGO with enhanced structural integrity. The use of microorganisms offers a sustainable approach, utilizing renewable carbon sources and mild reaction conditions. This study investigates the production of RGO using three different bacterial strains: (), (), and () and evaluates its toxicity for safe utilization. The aim is to assess the quality of the produced RGO and evaluate its toxicity for potential applications. Thus, this study focused on the microbial production of reduced graphene oxides well as the investigation of their cellular interactions. Graphite-derived graphene oxide was used as a starting material and microbially reduced GO products were characterized using the FTIR, Raman, XRD, TGA, and XPS methods to determine their physical and chemical properties. FTIR shows that the epoxy and some of the alkoxy and carboxyl functional groups were reduced by and , whereas the alkoxy groups were mostly reduced by . The / ratio from Raman spectra was found as 2.41 for GO. A substantial decrease in the ratio as well as defects was observed as 1.26, 1.35, and 1.46 for ERGO, LLRGO, and LPRGO after microbial reduction. The XRD analysis also showed a significant reduction in the interlayer spacing of the GO from 0.89 to 0.34 nm for all the reduced graphene oxides. TGA results showed that reduction of GO with provided more reduction than other bacteria and formed a structure closer to graphene. Similarly, analysis with XPS showed that L lactis provides the most effective reduction with a C/O ratio of 3.70. In the XPS results obtained with all bacteria, it was observed that the C/O ratio increased because of the microbial reduction. Toxicity evaluations were performed to assess the biocompatibility and safety of the produced RGO. Cell viability assays were conducted using DLD-1 and CHO cell lines to determine the potential cytotoxic effects of RGO produced by each bacterial strain. Additionally, apoptotic, and necrotic responses were examined to understand the cellular mechanisms affected by RGO exposure. The results indicated that all the RGOs have concentration-dependent cytotoxicity. A significant amount of cell viability of DLD-1 cells was observed for reduced graphene oxide. However, the highest cell viability of CHO cells was observed for reduced graphene oxide. All reduced graphene oxides have low apoptotic and necrotic responses in both cell lines. These findings highlight the importance of considering the specific bacterial strain used in RGO production as it can influence the toxicity and cellular response of the resulting RGO. The toxicity and cellular response to the final RGO can be affected by the particular bacterial strain that is employed to produce it. This information will help to ensure that RGO is used safely in a variety of applications, including tissue engineering, drug delivery systems, and biosensors, where comprehension of its toxicity profile is essential.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC10468768 | PMC |
http://dx.doi.org/10.1021/acsomega.3c03213 | DOI Listing |
Sci Rep
December 2024
Department of Computer Engineering, Marwadi University, Rajkot, 360003, India.
The contributed absorber design in graphene addition with the displacement of three materials for resonator design in Aluminum (Al), the middle substrate position with Titanium nitride (TiN), and the ground layer deposition by Iron (Fe) respectively. For the absorption validation highlight, the best four absorption wavelengths (µm) of 0.29, 0.
View Article and Find Full Text PDFNat Commun
December 2024
Department of Mechanical Engineering, Tsinghua University, Beijing, China.
Structural superlubricity (SSL), a state of ultralow friction and no wear between two solid surfaces in contact, offers a fundamental solution for reducing friction and wear. Recent studies find that the edge pinning of SSL contact dominates the friction. However, its nature remains mysterious due to the lack of direct characterizations on atomic scale.
View Article and Find Full Text PDFAdv Sci (Weinh)
December 2024
Hefei National Research Center for Physical Sciences at the Microscale, Department of Materials Science and Engineering, School of Chemistry and Materials Science, Key Laboratory of Precision and Intelligent Chemistry, University of Science and Technology of China, Hefei, Anhui, 230026, China.
High-temperature graphitization of graphene oxide (GO) is a crucial step for enhancing interlayer stacking and repairing the in-plane defects of reduced graphene oxide (rGO) films. However, the fine control of the structural repair and reducing the energy consumption in thermal treatment remain challenges. In this study, ab-initio molecular dynamics simulations combined with experiments are used to investigate the structural evolution of rGO upon thermal annealing, with or without the presence of single-layer graphene (SLG).
View Article and Find Full Text PDFNanotechnol Sci Appl
December 2024
Department of Nanobiotechnology, Institute of Biology, Warsaw University of Life Sciences, Warsaw, Poland.
Purpose: Biofilms are one of the main threats related to bacteria. Owing to their complex structure, in which bacteria are embedded in the extracellular matrix, they are extremely challenging to eradicate, especially since they can inhabit both biotic and abiotic surfaces. This study aimed to create an effective antibiofilm nanofilm based on graphene oxide-metal nanoparticles (GOM-NPs).
View Article and Find Full Text PDFFood Chem
December 2024
Food Engineering Technology Research Center/Key Laboratory of Henan Province, College of Food Science and Technology, Henan University of Technology, Lianhua Street, Zhengzhou 450001, China. Electronic address:
Most of the excessive aflatoxins in peanut oil are present at lower levels, and few photocatalysts have been reported for degrading low concentrations of aflatoxin B (AFB). This study employed aptamer-modified magnetic graphene oxide/titanium dioxide (MGO/TiO-aptamer) photocatalysts to degrade low concentrations of AFB in peanut oil, thoroughly investigating their selective efficiency, degradation mechanism, and product toxicity. The results indicated that the modification of aptamers on the surface of photocatalytic materials can enhance the selectivity of photocatalysts for AFB in peanut oil.
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!