Prelithiation is an essential technology to compensate for the initial lithium loss of lithium-ion batteries due to the formation of solid electrolyte interphase (SEI) and irreversible structure change. However, the prelithiated materials/electrodes become more reactive with air and electrolyte resulting in unwanted side reactions and contaminations, which makes it difficult for the practical application of prelithiation technology. To address this problem, herein, interphase engineering through a simple solution treatment after chemical prelithiation is proposed to protect the prelithiated electrode. The used solutions are carefully selected, and the composition and nanostructure of the as-formed artificial SEIs are revealed by cryogenic electron microscopy and X-ray photoelectron spectroscopy. The electrochemical evaluation demonstrates the unique merits of this artificial SEI, especially for the fluorinated interphase, which not only enhances the interfacial ion transport but also increases the tolerance of the prelithiated electrode to the air. The treated graphite electrode shows an initial Coulombic efficiency of 129.4%, a high capacity of 170 mAh g at 3 C, and negligible capacity decay after 200 cycles at 1 C. These findings not only provide a facile, universal, and controllable method to construct an artificial SEI but also enlighten the upgrade of battery fabrication and the alternative use of advanced electrolytes.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1002/smll.202305639 | DOI Listing |
Mater Horiz
January 2025
National local joint engineering research center for Lithium-ion Batteries and Materials Preparation Technology, Key Laboratory of Advanced Batteries Materials of Yunnan Province, Faculty of Metallurgical and Energy Engineering, Kunming University of Science and Technology, Kunming, 650093, China.
The stable operation of high-capacity lithium-sulfur batteries (LSBs) has been hampered by slow conversion kinetics of lithium polysulfides (LiPSs) and instability of the lithium metal anodes. Herein, 6-(dibutylamino)-1,3,5-triazine-2,4-thiol (DTD) is introduced as a functional additive for accelerating the kinetics of cathodic conversion and modulating the anode interface. We proposed that a coordination interaction mechanism drives the polysulfide conversion and modulates the Li solvated structure during the binding of the N-active site of DTD to LiPSs and lithium salts.
View Article and Find Full Text PDFJ Am Chem Soc
January 2025
School of Chemistry, Key Laboratory of Bio-Inspired Smart Interfacial Science and Technology of Ministry of Education, Beihang University, Beijing 100191, China.
Potassium (K)-based batteries hold great promise for cryogenic applications owing to the small Stokes radius and weak Lewis acidity of K. Nevertheless, energy-dense (>200 W h kg) K batteries under subzero conditions have seldom been reported. Here, an over 400 W h kg K battery is realized at -40 °C via an anode-free and dual-ion strategy, surpassing these state-of-the-art K batteries and even most Li/Na batteries at low temperatures (LTs).
View Article and Find Full Text PDFAngew Chem Int Ed Engl
January 2025
Key Laboratory of Advanced Energy Materials Chemistry, College of Chemistry, Weijin Road 94, 300071, Tianjin, CHINA.
Adv Sci (Weinh)
January 2025
Department of Materials Science, Fudan University, Shanghai, 200433, China.
Currently, lithium-ion batteries (LIBs) are at the forefront of energy storage technologies. Silicon-based anodes, with their high capacity and low cost, present a promising alternative to traditional graphite anodes in LIBs, offering the potential for substantial improvements in energy density. However, the significant volumetric changes that silicon-based anodes undergo during charge and discharge cycles can lead to structural degradation.
View Article and Find Full Text PDFACS Appl Mater Interfaces
January 2025
Research Center of Nano Science and Technology, College of Sciences, Shanghai University, Shanghai 200444, China.
The interfacial reaction of a silicon anode is very complex, which is closely related with the electrolyte components and surface elements' chemical status of the Si anode. It is crucial to elucidate the formation mechanism of the solid electrolyte interphase (SEI) on the silicon anode, which promotes the development of a stable SEI. However, the interface reaction mechanism on the silicon surface is closely related to the surface components.