It is well known that the development of lightweight alloys with improved comprehensive performance and application value are the future development directions for the ultra-high-strength 7xxx series Al-Zn-Mg-Cu alloys used in the aircraft field. As the lightest metal element in nature, lithium (Li) has outstanding advantages in reducing the density and increasing the elastic modulus in aluminum alloys, so Al-Zn-Mg-Cu alloys containing Li have gained widespread attention. Furthermore, since the Al-Zn-Mg-Cu alloy is usually strengthened by aging treatment, it is crucial to understand how Li addition affects its aging precipitation process. As such, in this article, the effects and mechanism of Li on the aging precipitation behavior and the impact of Li content on the aging precipitation phase of Al-Zn-Mg-Cu alloys are briefly reviewed, and the influence of Li on the service properties, including mechanical properties, wear resistance, and fatigue resistance, of Al-Zn-Mg-Cu alloys are explained. In addition, the corresponding development prospects and challenges of the Al-Zn-Mg-Cu-Li alloy are also proposed. This review is helpful to further understand the role of Li in Al-Zn-Mg-Cu alloys and provides a reference for the development of high-strength aluminum alloys containing Li with good comprehensive properties.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC10342766PMC
http://dx.doi.org/10.3390/ma16134750DOI Listing

Publication Analysis

Top Keywords

al-zn-mg-cu alloys
24
aging precipitation
16
alloys
9
precipitation process
8
aluminum alloys
8
al-zn-mg-cu
7
aging
5
role lithium
4
lithium aging
4
precipitation
4

Similar Publications

Effect of Stress Aging on Strength, Toughness and Corrosion Resistance of Al-10Zn-3Mg-3Cu Alloy.

Materials (Basel)

January 2025

Shandong Zhuoyue Precision Industry Group Co., Ltd., Jining 272114, China.

The 7000 series aluminum alloy represented by Al-Zn-Mg-Cu has good strength and toughness and is widely used in the aerospace field. However, its high Zn content results in poor corrosion resistance, limiting its application in other fields. In order to achieve the synergistic improvement of both strength and corrosion resistance, this study examines the response of strength, toughness and corrosion resistance of a high-strength aluminum alloy tail frame under aging conditions with external stresses of 135 MPa, 270 MPa and 450 MPa.

View Article and Find Full Text PDF

The presence of AlCuFe particles, formed due to Fe impurities in Al-Zn-Mg-Cu alloys, significantly impacts mechanical properties and formability, which is crucial for the use of these alloys in the automotive and aerospace industries. In this study, we prepared Al-Zn-Mg-Cu-based alloy sheets with large (LF), small (SF), and no (NF) AlCuFe particles to explore their effects on recrystallization and mechanical behavior. These sheets were fabricated using controlled cooling rates and subsequent thermo-mechanical processing.

View Article and Find Full Text PDF

Enhancing Stress Corrosion Cracking Resistance of Low Cu-Containing Al-Zn-Mg-Cu Alloys by Aging Treatment Control.

Materials (Basel)

November 2024

State Key Laboratory of Nonferrous Metals and Processes, GRINM Group Co., Ltd., Beijing 100088, China.

The 7085 aluminum alloy with a low Cu content is an important lightweight structural material in the aerospace field due to its advantages of low density, high specific strength, and high hardenability. However, like other high-strength Al-Zn-Mg-Cu alloys, this alloy is susceptible to stress corrosion cracking (SCC). Additionally, the lower Cu content may increase its tendency toward SCC, potentially impacting the safe use of this alloy.

View Article and Find Full Text PDF

The influence of as-cast grain size on recrystallization and the related mechanical properties of Al-Zn-Mg-Cu-based alloys was investigated. Grain sizes ranging from 163 to 26 μm were achieved by adding Ti, Cr and Mn, and ZnO nano-particles, which acted as heterogeneous nucleation sites. A decrease in the as-cast grain size led to a corresponding reduction in the recrystallized grain size from 54 to 13 μm.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!