Herein, micron-sized silver particles were prepared using the chemical reduction method by employing a Y-type microjet reactor, silver nitrate as the precursor, ascorbic acid as the reducing agent, and gelatin as the dispersion at room temperature (23 °C ± 2°C). Using a microjet reactor, the two reaction solutions collide and combine outside the reactor, thereby avoiding microchannel obstruction issues and facilitating a quicker and more convenient synthesis process. This study examined the effect of the jet flow rate and dispersion addition on the morphology and size of silver powder particles. Based on the results of this study, spherical and dendritic silver particles with a rough surface can be prepared by adjusting the flow rate of the reaction solution and gelatin concentration. The microjet flow rate of 75 mL/min and the injected gelatin amount of 1% of the silver nitrate mass produced spherical ultrafine silver particles with a size of 4.84 μm and a tap density of 5.22 g/cm.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC10058681PMC
http://dx.doi.org/10.3390/ma16062217DOI Listing

Publication Analysis

Top Keywords

silver particles
16
microjet reactor
12
flow rate
12
spherical ultrafine
8
ultrafine silver
8
y-type microjet
8
silver nitrate
8
silver
7
particles
5
preparation spherical
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!