The welding titanium cathode roller has the obvious advantages of low cost, high efficiency, and no diameter restriction. Unfortunately, the longitudinal weld on the cathode roller adversely impacts the quality of the electrolytic copper foil due to the great difference between the microstructure of the weld zone and the base metal. Thus, it is crucial to reduce their difference by regulating the microstructure of the weld zone. In this study, a novel complex treatment of heat treatment and sandblasting is primarily developed for regulating the microstructure of the weld zone. The results show that the novel complex treatment has an efficient effect on regulating the microstructure of the weld zone and making the microstructure in the weld zone close to that of the base metal. During vacuum annealing, the microstructure of the weld zone is refined to some degree, and 650 °C annealing has the optimal effect, which can effectively reduce the ratio of α phase's length to width and reduce the microstructure difference between the weld zone and the base metal. At the same time, with an increase in the annealing temperature, the tensile strength and yield strength decreased by about 10 MPa; the elongation after fracture increased by 20%; the average microhardness of the WZ and the HAZ decreased by about 10 HV; and that of the BM decreased by about 3 HV. The heat treatment after welding can effectively adjust the properties of the weld zone, reduce the hardness and strength, and improve the toughness. The subsequent sandblasting after annealing can further refine the grain size in the weld zone and make the microstructure in the weld zone close to that of the base metal. Sandblasting after annealing can further refine the grain in the weld zone and make the microstructure in the weld zone close to that of base metal. Meanwhile, an application test confirmed that the adverse impact of a longitudinal weld on the quality of electrolytic copper foil could be resolved by adopting this novel complex treatment. Therefore, this study provides valuable technical support for the "welding" manufacturing of the titanium sleeves of the cathode roller.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC10059315 | PMC |
http://dx.doi.org/10.3390/ma16062149 | DOI Listing |
Materials (Basel)
January 2025
Faculty of Materials Science and Technology, VŠB-Technical University of Ostrava, 17. listopadu 2172/15, 708 00 Ostrava, Czech Republic.
This paper summarizes the results of investigations into heterogeneous P23/P91 welds after long-term creep exposure at temperatures of 500, 550 and 600 °C. Two variants of welds were studied: In Weld A, the filler material corresponded to P91 steel, while in Weld B, the chemical composition of the consumable material matched P23 steel. The creep rupture strength values of Weld A exceeded those of Weld B at all testing temperatures.
View Article and Find Full Text PDFMaterials (Basel)
December 2024
School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, China.
TC17 titanium alloy is widely used in the aviation industry for dual-performance blades, and linear friction welding (LFW) is a key technology for its manufacturing and repair. However, accurate evaluation of the mechanical properties of TC17-LFW joints and research on their joint fracture behavior are still not clear. Therefore, this paper used the finite element numerical simulation method (FEM) to investigate the mechanical behavior of the TC17-LFW joint with a complex micro-structure during the tensile processing, and predicted its mechanical properties and fracture behavior.
View Article and Find Full Text PDFMaterials (Basel)
December 2024
School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China.
Forging additive hybrid manufacturing integrated the high efficiency of forging and the great flexibility of additive manufacturing, which has significant potential in the construction of reactor pressure vessels (RPVs). In the components, the heat-affected zone (HAZ, also called as bonding zone) between the forged substrate zone and the arc deposition zone was key to the final performance of the components. In this study, the Mn-Mo-Ni welding wire was deposited on the 16MnD5 substrate with a submerged arc heat source.
View Article and Find Full Text PDFMaterials (Basel)
December 2024
State Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, 92 West Dazhi Street, Harbin 15001, China.
This investigation focuses on Selective Laser Melting (SLM)-fabricated thin-walled Ta10W alloy components. Given the inherent limitations of SLM in producing large-scale, complex components in a single operation, laser welding was investigated as a viable secondary processing method for component integration. The study addresses the critical issue of weldability in additively manufactured tantalum-tungsten alloys, which frequently exhibit internal defects due to process imperfections.
View Article and Find Full Text PDFMaterials (Basel)
December 2024
Joining and Welding Research Institute, Osaka University, Osaka 567-0047, Japan.
Narrow-gap arc welding is an efficient method that significantly enhances industrial production efficiency and reduces costs. This study investigates the application of low-alloy steel wire EG70-G in narrow-gap gas metal arc welding (GMAW) on thick plates. Experimental observations were made to examine the arc behavior, droplet transition behavior, and weld formation characteristics of double-wire welding under various process parameters.
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!