Utilization of bottom ash waste as a granular column to enhance the lateral load capacity of soft kaolin clay soil.

Environ Sci Pollut Res Int

Faculty of Civil Engineering Technology, Universiti Malaysia Pahang, Lebuh Persiaran Tun Khalil Yaakob, 26300, Kuantan, Pahang, Malaysia.

Published: February 2023

AI Article Synopsis

  • Using bottom ash in ground improvement is a cost-effective and eco-friendly way to tackle problematic soils like soft kaolin clay, which often face various issues like severe settlement and low stability.
  • Research has shown that incorporating bottom ash columns can effectively improve the shear strength of kaolin clay, with specific optimal configurations resulting in up to 77% enhancement in strength.
  • The study involved extensive testing of various factors affecting the performance of these columns, leading to a prediction model that outlines how different dimensions and arrangements of bottom ash columns can maximize their effectiveness.

Article Abstract

Implementation of industrial wastes such as bottom ash in ground improvement can be cost-effective and environment-friendly. Ground improvement is an effective method of mitigation to improve problematic soils including soft kaolin clay soils as the problematic soils always expose to the severe settlements, low shear strength, immoderate plasticity, greater compressibility, dispersivity, bulging, erodibility, and susceptibility to climatic variables. Several studies conducted on the granular column using the bottom ash column. However, only a few studies have reported findings coherent with the statistical analysis. In this study, the lateral load capacity of bottom ash column-kaolin clay has been conducted. Coherently, the reinforced kaolin clay samples were tested via particle size distribution, Atterberg limit test, relative density, compaction test, permeability test, unconfined compression test, and unconsolidated undrained triaxial test with the single and group of encapsulated bottom ash columns with the geotextile encasement and a prediction model was developed. The effect of a number of columns, column diameter, column height, area replacement ratio, height penetration ratio, height-diameter column ratio, volume replacement ratio, and confining pressures on the shear strength of the single and group of encapsulated bottom ash columns have been investigated. The findings showed the effectiveness of using the bottom ash columns at various number of column, column diameter, column height, area replacement ratio, height penetration ratio, height-diameter column ratio, volume replacement ratio, and confining pressures can enhance the shear strength of the soil up to 77.00% at the optimal utilization of single encapsulated bottom ash column of 10-mm diameter and 80-mm height. Therefore, the study proved that the utilization of bottom ash waste as a granular column can significantly enhance the lateral load capacity of soft kaolin clay soil.

Download full-text PDF

Source
http://dx.doi.org/10.1007/s11356-023-25966-xDOI Listing

Publication Analysis

Top Keywords

bottom ash
36
kaolin clay
16
replacement ratio
16
column
12
granular column
12
lateral load
12
load capacity
12
soft kaolin
12
shear strength
12
encapsulated bottom
12

Similar Publications

Construction materials are significantly exposed to ecological hazards due to the presence of hazardous chemical constituents found in industrial and agricultural solid wastes. This study aims to investigate the use of sawdust particles (SDPs) and sawdust wastewater (SDW) in alkali-activated composites (AACs) made from a mixture of different silicon-aluminum-based solid wastes (slag powder-SP, red mud-RM, fly ash-FA, and carbide slag-CS). The study examines the impact of SDP content, treated duration of SDPs, and SDW content on both fresh and hardened properties of the AACs, including electrical conductivity, fluidity, density, flexural and compressive strengths, and drying shrinkage.

View Article and Find Full Text PDF

TiO-ZnO functionalized low-cost ceramic membranes from coal fly ash for the removal of tetracycline from water under visible light.

Discov Nano

January 2025

Materials Science Innovation and Modelling (MaSIM) Research Focus Area, Faculty of Natural and Agricultural Sciences, North-West University, Mafikeng Campus, Private Bag X2046, Mmabatho, 2735, South Africa.

Hybrid wastewater treatment systems offer viable solutions to enhance the removal of complicated contaminants from aqueous system. This innovation has opened new avenues for advanced wastewater treatment processes. Herein, a novel TiO-ZnO functionalized coal fly ash-based ceramic membrane was fabricated by utilizing a combined pressing and sintering method.

View Article and Find Full Text PDF

The study aimed to explore the potential use of coal-fired power plant bottom ashes in Pleurotus ostreatus cultivation using spent coffee grounds. The study analyzed five compositions of growth substrate for mushrooms: pure coffee grounds (I) as a control sample; coffee grounds substrate with the addition of 1% (II); 5% (III); 10% (IV) bottom ash; and bottom ash alone (V). The study revealed that compared to the control sample (I), the addition of 1% bottom ash (II) did not affect the time of mycelium growth but slowed fruiting body growth by 4 days.

View Article and Find Full Text PDF

Secondary aluminum dross self-heating enhances hazardous waste vitrification.

Waste Manag

December 2024

School of Environmental Science and Engineering, Zhejiang Provincial Key Laboratory of Solid Waste Treatment and Recycling, Zhejiang Engineering Research Center of Non-ferrous Metal Waste Recycling, Zhejiang Gongshang University, Hangzhou, Zhejiang 310012, China. Electronic address:

This study demonstrates the potential of secondary aluminum dross (SAD) to enhance the vitrifying hazardous waste incineration fly ash (FA) and bottom slag (BS). Based on the CaO-SiO-AlO ternary phase diagram, a liquid phase can be achieved at relatively low temperatures by carefully adjusting the AlO content, particularly when the CaO to SiO ratio is around 0.66.

View Article and Find Full Text PDF

Effects of Nanosilica on the Properties of Ultrafine Cement-Fly Ash Composite Cement Materials.

Nanomaterials (Basel)

December 2024

School of Civil Engineering and Architecture, Henan University, Kaifeng 475000, China.

The increasing incidence of structural failures, such as cracks and collapses, in rock masses within mines, tunnels, and other civil engineering environments has attracted considerable attention among scholars in recent years. Grouting serves as a principal solution to these issues. The Renlou Coal Mine in the Anhui Province is used as a case study to evaluate the effectiveness of nanosilica (NS) as an additive in ultrafine cement (UC), introducing a novel grouting material for practical applications.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!