Severity: Warning
Message: file_get_contents(https://...@pubfacts.com&api_key=b8daa3ad693db53b1410957c26c9a51b4908&a=1): Failed to open stream: HTTP request failed! HTTP/1.1 429 Too Many Requests
Filename: helpers/my_audit_helper.php
Line Number: 176
Backtrace:
File: /var/www/html/application/helpers/my_audit_helper.php
Line: 176
Function: file_get_contents
File: /var/www/html/application/helpers/my_audit_helper.php
Line: 250
Function: simplexml_load_file_from_url
File: /var/www/html/application/helpers/my_audit_helper.php
Line: 1034
Function: getPubMedXML
File: /var/www/html/application/helpers/my_audit_helper.php
Line: 3152
Function: GetPubMedArticleOutput_2016
File: /var/www/html/application/controllers/Detail.php
Line: 575
Function: pubMedSearch_Global
File: /var/www/html/application/controllers/Detail.php
Line: 489
Function: pubMedGetRelatedKeyword
File: /var/www/html/index.php
Line: 316
Function: require_once
Natural fibres have been partly substituting synthetic fibres in polymer composites due to their renewable character and many other advantages, and sometimes, they can be hybridized into a single composite for a better combination of properties. This work aims to study the effect of hybridization and stacking sequence on the mechanical and physical properties of the glass/jute laminates. For that, pure jute, pure glass and glass/jute hybrids were manufactured by vacuum infusion process using orthophthalic polyester resin. The composites were characterized via C-scan analysis, density, volume fraction of constituents and optical microscopy analyses. Mechanical properties were obtained from tensile, compression and shear tests. The longitudinal properties were higher than transverse properties for all laminates. The hybrids presented intermediate density and mechanical properties compared to pure glass and pure jute laminates. The hybrids produced similar density and tensile modulus, but with small differences in tensile strength and compressive strength which were justified based on variations in resin and void content due to the influence of the stacking sequence (glass/jute interlayer regions). In addition, the pure glass and the hybrid laminates displayed acceptable failure morphology in the in-plane shear test, but not the pure jute laminate.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC9655998 | PMC |
http://dx.doi.org/10.3390/polym14214742 | DOI Listing |
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!