Zirconia restorations, which are fabricated by additive 3D gel deposition and do not require glazing like conventional restorations, were introduced as "self-glazed" zirconia restorations into dentistry. This in vitro investigation characterized the surface layer, microstructure and the fracture and aging behavior of "self-glazed" zirconia (Y-TZP) three-unit fixed dental prostheses (FDP) and compared them to conventionally CAD/CAM milled and glazed controls (Y-TZP-FDPs). For this purpose, the FDPs were analyzed by (focused ion beam) scanning electron microscopy, laserscanning microscopy, energy dispersive X-ray spectroscopy, X-ray diffraction and a dynamic and static loading test. For the latter, half of the samples of each material group (n = 16) was subjected to 5 million cycles of thermocyclic loading (98N) in an aqueous environment in a chewing simulator. Afterwards, all FDPs were loaded to fracture. Y-TZP-FDPs demonstrated a comparable elemental composition but higher surface microstructural homogeneity and fracture strength compared to Y-TZP-FDPs. Microstructural flaws within the FDPs' surfaces were identified as fracture origins. The high fracture strength of the Y-TZP-FDPs was attributed to a finer-grained microstructure with fewer surface flaws compared to the Y-TZP-FDPs which showed numerous flaws in the glaze overlayer. A decrease in fracture strength after dynamic loading from 5165N to 4507N was observed for the Y-TZP-FDPs, however, fracture strength remained statistically significantly above the one measured for Y-TZP-FDPs (before chewing simulation: 1923N; after: 2041N). Within the limits of this investigation, it can therefore be concluded that Y-TZP appears to be stable for clinical application suggesting further investigations to prove clinical applicability.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1016/j.jmbbm.2022.105456 | DOI Listing |
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!