Vickers indentation (IF) and single-edge-V-notched beam (SEVNB), to measure the fracture toughness (K ) of zirconia-based dental ceramics and mathematical models were proposed to establish a correlation between both. Zirconia (ZrO ) stabilized with 3 mol. % of Y O (3Y-TZP) and 5 mol% of Y O (5Y-PSZ) were compacted (n = 42) and sintered for 2 h at different temperatures (1475°C, 1500°C, 1550°C, or 1600°C). After sintering, they were characterized by relative density using the ASTM C373-88 standard, X-ray diffraction (XRD) and scanning electron microscopy (SEM). The average grain size was measured according to the ASTM E1382-97 standard. The fracture toughness (K ) was determined using two methods: Vickers indentation fracture toughness (K ): method based on mathematical modeling that considers the parameters used for the Vickers hardness test and Fracture toughness by the single-edge-V-notch-beam (K ): method proposed by ISO 23146:08. The main phases of the 3Y-TZP and 5Y-PSZ ceramics were ZrO -tetragonal and ZrO -cubic, respectively. The 3Y-TZP specimens showed equiaxed grains with average grain sizes ranging from 0.55 to 0.79 μm. The grain sizes of 5Y-PSZ of specimens sintered at 1475°C and 1600°C were 0.62 and 2.32 μm, respectively. For all ceramics the crack size ratio was c/a < 2.5, suggesting a Palmqvist-type crack system. The fracture toughness measured by the Vickers indentation method (K ) and by the SEVNB method (K ) was the same when the experimental data were fit to a mathematical model.

Download full-text PDF

Source
http://dx.doi.org/10.1002/jbm.b.35137DOI Listing

Publication Analysis

Top Keywords

fracture toughness
20
dental ceramics
8
vickers indentation
8
average grain
8
grain sizes
8
toughness
5
comparison fracture
4
toughness techniques
4
techniques zirconia
4
zirconia dental
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!