A PHP Error was encountered

Severity: Warning

Message: file_get_contents(https://...@pubfacts.com&api_key=b8daa3ad693db53b1410957c26c9a51b4908&a=1): Failed to open stream: HTTP request failed! HTTP/1.1 429 Too Many Requests

Filename: helpers/my_audit_helper.php

Line Number: 176

Backtrace:

File: /var/www/html/application/helpers/my_audit_helper.php
Line: 176
Function: file_get_contents

File: /var/www/html/application/helpers/my_audit_helper.php
Line: 250
Function: simplexml_load_file_from_url

File: /var/www/html/application/helpers/my_audit_helper.php
Line: 3122
Function: getPubMedXML

File: /var/www/html/application/controllers/Detail.php
Line: 575
Function: pubMedSearch_Global

File: /var/www/html/application/controllers/Detail.php
Line: 489
Function: pubMedGetRelatedKeyword

File: /var/www/html/index.php
Line: 316
Function: require_once

Photoinitiator Selection and Concentration in Photopolymer Formulations towards Large-Format Additive Manufacturing. | LitMetric

Photopolymers are an attractive option for large-format additive manufacturing (LFAM), because they can be formulated from structural thermosets and cure rapidly in ambient conditions under low-energy ultraviolet light-emitting diode (UV LED) lamps. Photopolymer cure is strongly influenced by the depth penetration of UV light, which can be limited in the 2-4 mm layer thicknesses typical of LFAM. Photoinitiator (PI) systems that exhibit photobleaching have proven useful in thick-section cure applications, because they generate a photoinitiation wavefront, but this effect is time-dependent. This study investigates the light transmission and through-thickness cure behavior in (meth)acrylate photopolymer formulations with the photobleaching initiator bis(2,4,6-trimethylbenzoyl)-phenylphosphine oxide (BAPO). Utilizing an optical model developed by Kenning et al., lower concentrations (0.1 wt% to 0.5 wt%) of BAPO were predicted to yield rapid onset of photoinitiation. In situ cure measurements under continuous UV LED irradiation of 380 mW/cm showed that a 0.1 wt% concentration of BAPO achieved peak polymerization rate within 2.5 s at a 3-mm depth. With only 1 s of irradiation at 1.7 W/cm intensity, the 0.1 wt% BAPO formulation also achieved the highest level of cure of the formulas tested. For an irradiation dose of 5.5 J/cm at a duration of 3.7 s, cured polymer specimens achieved a flexural strength of 108 MPa and a flexural modulus of 3.1 GPa. This study demonstrates the utility of optical modeling as a potential screening tool for new photopolymer formulations, primarily in identifying an upper limit to PI concentration for the desired cure depth. The results also show that photobleaching provides only a limited benefit for LFAM applications with short (1.0 s to 3.7 s) UV irradiation times and indicate that excess PI concentration can inhibit light transmission even under extended irradiation times up to 60 s.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC9268840PMC
http://dx.doi.org/10.3390/polym14132708DOI Listing

Publication Analysis

Top Keywords

photopolymer formulations
12
large-format additive
8
additive manufacturing
8
light transmission
8
wt% bapo
8
irradiation times
8
cure
7
irradiation
5
photoinitiator selection
4
concentration
4