This study simulated the after-burned zirconium cladding oxidation in air at temperatures between 500 and 800 °C. The weight changes of Zircaloy-4 cladding with hydrogen contents of 100-1000 ppm continuously measured through thermogravimetric analysis (TGA) during oxidation tests at different temperatures in an air atmosphere. The TGA results indicate a transition of oxidation kinetics from a parabolic rate law to a linear rate law for as-received and hydrided Zircaloy-4 cladding. The hydrogen concentration of Zircaloy-4 had a marked effect on its pre-transition oxidation in air between 500 and 800 °C. For all samples, the linear oxidation (post transition stage) at 650 °C, which is the critical oxidation temperature, displays a similar trend. In addition, scanning electron microscopy and transmission electron micros-copy examinations indicated the presence of a few and numerous discontinuous micro-cracks in the oxide layer in the pre-transition and post-transition stages, respectively.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC9100136PMC
http://dx.doi.org/10.3390/ma15092997DOI Listing

Publication Analysis

Top Keywords

zircaloy-4 cladding
12
cladding hydrogen
12
oxidation air
8
500 800
8
800 °c
8
rate law
8
oxidation
7
oxidation behavior
4
behavior characterization
4
zircaloy-4
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!