Purpose: The physical and mechanical performance of a newly commercialized dental restorative material (alkasite) was compared with glass ionomer cement (GIC) and nano-hybrid composite.

Methodology: Human extracted premolars were used to investigate the shear bond strength. Restorative materials were placed on the dentine surface and were aged in deionized water for 14 days. The 3-D surface roughness was evaluated before and after chewing simulation cycles (50,000). The samples were fatigued mechanically using a chewing simulator and investigated with a scanning electron microscope (SEM).

Results: For shear bond strength, alkasite showed significantly high values than GIC, whereas non-significant difference was observed between alkasite and nano-hybrid composite. After the chewing simulation (50,000 cycles), non-significant difference was found between GIC and nano-hybrid composite, where surface roughness values were highest for GIC and lowest for alkasite.

Conclusion: The newly developed restorative material (alkasite) has shown better results than existing restorative materials.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC8589597PMC
http://dx.doi.org/10.1016/j.sdentj.2020.04.012DOI Listing

Publication Analysis

Top Keywords

restorative materials
12
restorative material
8
material alkasite
8
gic nano-hybrid
8
shear bond
8
bond strength
8
surface roughness
8
chewing simulation
8
non-significant difference
8
nano-hybrid composite
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!