Aims And Objectives: The purpose of this study is to evaluate the surface topography of gutta-percha (GP) after disinfecting with sodium hypochlorite (NaOCl) (5.25%), silver nanoparticles (AgNPs) (70 µg/ml), and chitosan nanoparticles (ChNPs) (1.5 mg/ml) by atomic force microscopy (AFM).
Materials And Methods: Forty GP cones were taken in this study. These samples were divided into four different groups such as Group I - control group (untreated GP Points) and Group II, III, and IV were treated with 5.25% NaOCl, 70 µg/ml AgNPs, and 1.5 mg/ml ChNPs, respectively. The surface topography analysis of the samples was performed using AFM.
Statistical Analysis: Root mean square (RMS) and surface roughness parameters were used to compare the structure of GP points with contact mode imaging. These values were tested by IBM SPSS-20.0 version statistical software using one-way ANOVA and (Tukey's honestly significant difference) tests. They were considered statistically significant when < 0.05.
Results: The RMS and surface roughness values are significantly higher for NaOCl group (5.25% NaOCl) when compared with AgNPs group (70 µg/ml AgNPs) and ChNPs group (1.5 mg/ml ChNPs).
Conclusion: This study has shown more surface topography deterioration of GP treated with NaOCl and lesser deterioration with AgNPs and ChNPs which affects postoperative prognosis.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC8378490 | PMC |
http://dx.doi.org/10.4103/JCD.JCD_505_20 | DOI Listing |
Dent Mater
January 2025
Department of Materials, School of Natural Sciences, University of Manchester, Manchester M13 9PL, UK; Photon Science Institute, University of Manchester, Manchester M13 9PL, UK. Electronic address:
Objective: To assess the impact of mechanical decontamination using rotary brushes on the surface topography, elemental composition, roughness, and wettability of titanium implant surfaces.
Methods: Four commercially available rotary brushes were used: Labrida BioClean Brush® (LB), i-Brush1 (IB), NiTiBrush Nano (NiTiB), and Peri-implantitis Brush (PIB). Seventy-five titanium discs with sandblasted, large-grit, acid-etched (SLA) surfaces were randomly assigned to five groups (n = 15): LB, IB, NiTiB, PIB, and a control group.
Tribol Int
May 2024
Department of Bioengineering, University of Pittsburgh, 3700 O'Hara St., Benedum Hall Room 302, Pittsburgh, PA 15261.
Roughness metrics measured with stylus profilometry are commonly used to explain a floor's friction performance, yet these metrics inconsistently predict shoe-floor friction. While strong correlations have been shown for systematically modified flooring, the goal of this study is to address a gap regarding the predictive ability of these metrics across heterogeneous porcelain flooring products. The predictive ability of four roughness metrics on oily friction performance was assessed using 23 floors and 4 shoe designs.
View Article and Find Full Text PDFACS Appl Mater Interfaces
January 2025
Institute of Optical Functional Materials for Biomedical Imaging, School of Chemistry and Pharmaceutical Engineering, Shandong First Medical University & Shandong Academy of Medical Science, Taian, Shandong 271016, PR China.
Photoactivatable gold nanocarriers are transforming antitumor therapies by leveraging their distinctive physicochemical properties, enabling targeted drug delivery and enhanced therapeutic efficacy in cancer treatment. This study systematically investigates how surface topography and morphology of gold nanocarriers influence drug loading capacity, light-to-heat conversion efficiency, and overall therapeutic performance in photo/chemotherapy. We synthesized four distinct morphologies of gold nanoparticles: porous gold nanocups (PAuNCs), porous gold nanospheres (PAuNSs), solid gold nanocups (SAuNCs), and solid gold nanospheres (SAuNSs).
View Article and Find Full Text PDFLangmuir
January 2025
Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang 110819, China.
The stick-slip phenomenon as a prevalent friction instability poses significant challenges to industry, including frictional vibration, reduced precision, and noise generation. The interfacial interactions between asperities on the surface of materials are critical in influencing stick-slip behavior. This study focused on modifying the asperities on the surface of zinc-coated steel through temper rolling as a new approach to suppress friction-induced stick-slip vibration and noise.
View Article and Find Full Text PDFBraz Oral Res
January 2025
Universidade Federal da Paraíba - UFPB, Health Science Center Department of Clinical and Community Dentistry, João Pessoa, PB, Brazil.
This study aimed to evaluate the effectiveness of bioactive toothpastes in remineralizing eroded enamel surfaces in vitro. Bovine enamel blocks (n = 48) were obtained and classified into untreated, demineralized, and treated areas. Specimens were randomly classified into six groups (n = 8 each): fluoride-free toothpaste (NCT), Colgate Total 12 (PCT), Sensodyne Repair and Protect (SRP), Sensodyne Pronamel (SPE), Regenerador + Sensitive (RGS), and RGS/calcium booster (RCB).
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!