Severity: Warning
Message: file_get_contents(https://...@pubfacts.com&api_key=b8daa3ad693db53b1410957c26c9a51b4908&a=1): Failed to open stream: HTTP request failed! HTTP/1.1 429 Too Many Requests
Filename: helpers/my_audit_helper.php
Line Number: 176
Backtrace:
File: /var/www/html/application/helpers/my_audit_helper.php
Line: 176
Function: file_get_contents
File: /var/www/html/application/helpers/my_audit_helper.php
Line: 250
Function: simplexml_load_file_from_url
File: /var/www/html/application/helpers/my_audit_helper.php
Line: 1034
Function: getPubMedXML
File: /var/www/html/application/helpers/my_audit_helper.php
Line: 3152
Function: GetPubMedArticleOutput_2016
File: /var/www/html/application/controllers/Detail.php
Line: 575
Function: pubMedSearch_Global
File: /var/www/html/application/controllers/Detail.php
Line: 489
Function: pubMedGetRelatedKeyword
File: /var/www/html/index.php
Line: 316
Function: require_once
In this study, (R)-9-(2-hydroxy propyl)adenine (HPA) is the molecule of interest for investigation. The XRD from single crystal of HPA has been used to extract its structural features. Since HPA crystallised in a non-centro symmetric space group P222, its NLO property was studied and it was found to exhibit very good SHG activity. To explore the intermolecular interactions the generated Hirshfeld surface has been investigated along with 2D-fingerprint plots. The experimental electronic and NMR spectra taken in the UV-visible and radio frequency regions respectively for HPA have been corroborated in correlation with theoretical predictions at Density Function Theory using 6-311++g (d, p) basis set. The experimental XRD geometrical parameters, chemical shifts of C and H and λ values of HPA fit satisfactorily with the corresponding theoretically obtained numerical values as well as the stimulated spectrograms with the experimental ones. Further to explore the electronic structure, the MESP surface has been generated and investigated. The thermodynamic, kinetic and chemical reactivity features have been explored by means of frontier molecular orbitals of HPA.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC8102761 | PMC |
http://dx.doi.org/10.1016/j.heliyon.2021.e06593 | DOI Listing |
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!