Size effects and structural modifications in amorphous TiO films deposited by atomic layer deposition (ALD) were investigated. As with the previously investigated ALD-deposited AlO system we found that the film's structure and properties are strongly dependent on its thickness, but here, besides the significant change in the density of the films there is also a change in their chemical state. The thin near-surface layer contained a significantly larger amount of Ti species and oxygen vacancies relative to the sample's bulk. We attribute this change in chemistry to the ALD specific deposition process wherein each different atomic species is deposited in turn, thereby forming a "corundum-like" structure of the near-surface layer resembling that found in the AlO system. This, combined with the fact that each deposited layer starts out as a surface layer and maintains the surface structure over the next several following deposition cycles, is responsible for the overall decrease in the film density. This is the first time this effect has been shown in detail for TiO, expending the previously discovered phenomenon to a new system and demonstrating that while similar effects occur, they can present in different ways for oxide systems with different structures and symmetries.

Download full-text PDF

Source
http://dx.doi.org/10.1039/d1cp00341kDOI Listing

Publication Analysis

Top Keywords

surface structure
8
atomic layer
8
layer deposition
8
alo system
8
near-surface layer
8
layer
6
retention surface
4
structure
4
structure lower
4
lower density
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!