Can polylactic acid be a CAD/CAM material for provisional crown restorations in terms of fit and fracture strength?

Dent Mater J

Dental Materials Unit, Center for Dental and Oral Medicine Clinic for Fixed and Removable Prosthodontics and Dental Materials Science, University of Zürich.

Published: May 2021

This study aimed to evaluate polylactic acid (PLA) as a provisional crown material. Lower right first molar phantom tooth was used for the fabrication of 60 crowns. Samples were divided into three groups (n=20) according to the material: Group PL (PLA), Group PM (polymethyl methacrylate), and Group PE (polyetheretherketone). Each group was investigated for internal and marginal fit, fracture strength, and fracture mode. Data were analyzed using ANOVA, chi-squared test, and Tukey's tests (p≤0.05). The average marginal gap value of each group was: PE 56.00±4.67 µm, PM 61.15±4.44 µm, and PL 60.40±2.85 µm (p<0.001). The average internal gap value for each group was: PE 128.90±8.39 µm, PM 132.40±7.51 µm, and PL 130.75±9.76 µm (p=0.442). The average fracture strength of each group was: PE 840.90±13.23 N, PM 733.30±9.00 N, and PL 664.50±10.79 N (p<0.001). Results demonstrated that PLA may be a good option as a provisional crown material.

Download full-text PDF

Source
http://dx.doi.org/10.4012/dmj.2020-232DOI Listing

Publication Analysis

Top Keywords

polylactic acid
8
provisional crown
8
fit fracture
8
group
5
acid cad/cam
4
cad/cam material
4
material provisional
4
crown restorations
4
restorations terms
4
terms fit
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!