Aim: To investigate the colour stability of Crystalized Acetyl Resin, in comparison to three other aesthetic restorative materials, when immersed in different staining aqueous solutions.

Materials And Methods: Fifteen disc-shaped specimens each, of the four materials tested, were immersed in either DW or 4 staining solutions. CIE L*a*b* values were recorded using a digital spectrophotometer on a weekly basis for 4 weeks. Data were compared using three- way/two-way ANOVA along with auto-regressive model.

Results: Two-way Anova indicates that there is a significant colour change in all materials over time when immersed in the different staining solutions. Auto-regressive model showed that the colour change in each successive week was statistically significant (P < 0.001).

Conclusion: The most staining solution affecting the materials during this study was black coffee. Within the limitation of this study, Acetyl Resin was the most colour stable material among the other materials.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC7904845PMC
http://dx.doi.org/10.1038/s41405-020-00055-0DOI Listing

Publication Analysis

Top Keywords

immersed staining
12
colour stability
8
acetyl resin
8
restorative materials
8
staining solutions
8
colour change
8
colour
4
stability crystallized
4
crystallized acetyl
4
resin material
4

Similar Publications

Objective: This study aimed to evaluate the in vitro effects of coffee exposure on the color and roughness of conventional and bulk-fill resin composites, with and without surface pre-reacted glass-ionomer (S-PRG) filler.

Methodology: Forty-eight cylindrical samples (Ø6 mm × 2 mm) were prepared and categorized as follows (n = 12 per group): conventional nano-hybrid (Tetric N-Ceram, Ivoclar); nano-hybrid with S-PRG filler (Beautifil II, Shofu); bulk-fill (Tetric N-Ceram Bulk Fill, Ivoclar); and bulk-fill with S-PRG filler (Beautifil Bulk Restorative, Shofu). The samples were assessed for surface roughness (Ra, μm), color coordinates (CIE Lb), and overall color change (ΔE, ΔE).

View Article and Find Full Text PDF

The Staining Susceptibility and Surface Roughness of Teeth Restored by Microabrasion and Resin Infiltration: An In Vitro Study.

Polymers (Basel)

December 2024

Department of Restorative Dentistry, Faculty of Dentistry, Thammasat University, 99 M. 18, Paholyothin Road, Klong Luang, Pathum Thani 12120, Thailand.

This study assessed the susceptibility to staining and surface roughness of white-spot lesions (WSLs) treated with resin infiltration (RIT) and microabrasion (MA) under simulated aging through thermocycling in red wine. Seventy-eight extracted human premolars with artificial WSLs were divided into three groups: untreated WSLs (control), RIT-treated (ICON, DMG), and MA-treated (Opalustre, Ultradent). Each group was further split: one subgroup immersed in artificial saliva and the other thermocycled in red wine.

View Article and Find Full Text PDF

Purpose: This study was aimed to compare the difference between iRoot SP and AH Plus on root canal sealing ability for teeth extracted due to severe periodontitis and explore whether the dentin tubule pathway plays an important role in the development of endodontic-periodontic lesions(EPL), in order to provide a theoretical basis for selection of proper time for root canal therapy and suitable root canal sealants in patients with EPL.

Methods: Fifty single-root anterior teeth extracted due to severe periodontitis were selected. The roots were completely debrided to remove the calculus, dental plaque and cementum.

View Article and Find Full Text PDF

Introduction: This study investigated the physical, mechanical, and optical properties of 3-dimensional (3D) printing resins compared with thermoplastic materials to evaluate their suitability for the fabrication of orthodontic clear retainers.

Methods: Samples were prepared from thermoplastic sheets (Duran [Scheu-Dental GmbH, Iserlohn, Germany] and Zendura [Bay Materials LLC, Fremont, Calif]) and biocompatible 3D-printing resins (Dental LT Clear V2 [Formlabs Inc, Somerville, Mass] and OrthoFlex [Nextdent BV, Soesterberg, The Netherlands]) according to the manufacturer's instructions. The materials were characterized by Fourier transform infrared spectroscopy, differential scanning calorimetry, and water sorption tests.

View Article and Find Full Text PDF

Mechanical properties and integrity of biodegradable Zn alloys during degradation holds significant importance. In this study, a Zn-Mg-Mn alloy with tensile strength of 414 MPa and an elongation of 26% was developed. The strength contributions of as-extruded Zn alloy from grain boundary strengthening, precipitation strengthening, and second phase strengthening.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!