In this study, we focused on obtaining polysulfone-polyurethane (PSF-PUR) blend partly degradable hollow fiber membranes (HFMs) with different compositions while maintaining a constant PSF:PUR = 8:2 weight ratio. It was carried out through hydrolysis, and evaluation of the properties and morphology before and after the hydrolysis process while maintaining a constant cut-off. The obtained membranes were examined for changes in ultrafiltration coefficient (UFC), retention, weight loss, morphology assessment using scanning electron microscopy (SEM) and MeMoExplorer™ Software, as well as using the Fourier-transform infrared spectroscopy (FT-IR) method. The results of the study showed an increase in the UFC value after the hydrolysis process, changes in retention, mass loss, and FT-IR spectra. The evaluation in MeMoExplorer™ Software showed the changes in membranes' morphology. It was confirmed that polyurethane (PUR) was partially degraded, the percentage of ester bonds has an influence on the degradation process, and PUR can be used as a pore precursor instead of superbly known polymers.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC7828234PMC
http://dx.doi.org/10.3390/membranes11010051DOI Listing

Publication Analysis

Top Keywords

psf-pur blend
8
hollow fiber
8
properties morphology
8
morphology hydrolysis
8
maintaining constant
8
hydrolysis process
8
memoexplorer™ software
8
chemical degradation
4
degradation psf-pur
4
blend hollow
4

Similar Publications

This work was focused on biodegradation with bacteria studies of PSF-PUR blend semipermeable hollow fiber membranes that possibly can undergo a partial degradation process. Hollow fiber membranes were obtained from polysulfone (PSF) and polyurethane (PUR) containing ester bonds in the polymer chain in various weight ratios using two solvents: ,-Dimethylmethanamide (DMF) or -Methylpyrrolidone (NMP). The membranes that underwent the biodegradation process were tested for changes in the ultrafiltration coefficient (UFC), retention and cut-off point.

View Article and Find Full Text PDF

In this study, we focused on obtaining polysulfone-polyurethane (PSF-PUR) blend partly degradable hollow fiber membranes (HFMs) with different compositions while maintaining a constant PSF:PUR = 8:2 weight ratio. It was carried out through hydrolysis, and evaluation of the properties and morphology before and after the hydrolysis process while maintaining a constant cut-off. The obtained membranes were examined for changes in ultrafiltration coefficient (UFC), retention, weight loss, morphology assessment using scanning electron microscopy (SEM) and MeMoExplorer™ Software, as well as using the Fourier-transform infrared spectroscopy (FT-IR) method.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!