Gold bioleaching mediated by iodide oxidizing bacteria (IOB) has been proposed as a sustainable alternative to conventional technologies such as cyanidation. This study evaluated the ability of two IOB sourced from a commercial culture collection, () DSM 11457 and DSM 17069, to bioleach gold from electronic waste (e-waste) (1030 ppm gold) and sulfidic gold ore concentrate (45 ppm gold) using one-step, two-step and spent medium leaching at 1% pulp density over 10 days. Two-step bioleaching of ore concentrate resulted in the highest gold leaching yields (approximately ~100% and 34% for and , respectively), followed by spent medium leaching and one-step leaching. The yields remained low for e-waste with both strains (maximum 0.93% and 1.6% for and , respectively) and decreased over time, likely due to the instability of the solubilized gold at relatively low redox potentials (<300 mV vs. Ag/AgCl). Another limiting factor may be the partial inhibition of bacterial growth in the presence of the ore concentrate and e-waste. Therefore, future studies should evaluate the pre-treatment of the ore concentrate and e-waste to remove inhibitory and oxidant consuming compounds before bioleaching with IOB to optimize leaching yields.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC7696734 | PMC |
http://dx.doi.org/10.3390/microorganisms8111783 | DOI Listing |
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!