A digital etching method was proposed to achieve excellent control of etching depth. The digital etching characteristics of p-Si and SiGe using a combination of HNO oxidation and buffered oxide etching oxide removal processes were investigated. Experimental results showed that oxidation saturates as time goes on because of low activation energy and its diffusion-limited characteristic. An oxidation model was developed to describe the wet oxidation process with nitric acid. The model was calibrated with experimental data, and the oxidation saturation time, final oxide thickness, and selectivity between SiGe and p-Si were obtained. In SiGe/p-Si stacks, the saturated relative etched depth per cycle was 0.5 nm (four monolayers), and variation between experiments was about 4% after saturation. A corrected selectivity calculation formula was also proposed, and the calculated selectivity was 3.7-7.7 for different oxidation times, which was the same as the selectivity obtained from our oxidation model. The proposed model can be used to analyze process variations and repeatability, and it can provide credible guidance for the design of other wet digital etching experiments.

Download full-text PDF

Source
http://dx.doi.org/10.1021/acsami.0c14018DOI Listing

Publication Analysis

Top Keywords

digital etching
16
oxidation model
8
oxidation
7
etching
6
selective digital
4
etching silicon-germanium
4
silicon-germanium nitric
4
nitric hydrofluoric
4
hydrofluoric acids
4
acids digital
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!