We analyzed the effects of pyrolysis temperature and duration on the physiochemical properties and Cd(II) adsorption capacity of spent tea leaves (STL) biochar. The STL biochar was produced by pyrolysis at 300, 400, 500 and 600 °C for 1 and 2 h. The pyrolysis temperature was positively correlated to the ash content, pH, electrical conductivity, specific surface area (S), pore volume (PV) and C content, and negatively with the total yield, O, H and N content, and the O/C and H/C atomic ratios. Furthermore, the surface porosity of STL biochar increased, the density of oxygen-containing functional groups decreased, and the formation of aromatic structures was enhanced at higher pyrolysis temperatures. The adsorption of Cd(II) onto STL biochar fitted with the pseudo-second-order kinetics and Langmuir isotherms model. The STL biochar produced at 600 °C for 2 h showed the maximum Cd(II) adsorption capacity of 97.415 mg/g. In addition, Cd(II) adsorption was mainly physical and occurred in monolayers. Thus, STL biochar is a suitable low-cost adsorbent for wastewater treatment.

Download full-text PDF

Source
http://dx.doi.org/10.2166/wst.2020.309DOI Listing

Publication Analysis

Top Keywords

stl biochar
24
cdii adsorption
16
adsorption capacity
12
temperature duration
8
spent tea
8
tea leaves
8
physiochemical properties
8
properties cdii
8
pyrolysis temperature
8
biochar produced
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!