A PHP Error was encountered

Severity: Warning

Message: file_get_contents(https://...@pubfacts.com&api_key=b8daa3ad693db53b1410957c26c9a51b4908&a=1): Failed to open stream: HTTP request failed! HTTP/1.1 429 Too Many Requests

Filename: helpers/my_audit_helper.php

Line Number: 176

Backtrace:

File: /var/www/html/application/helpers/my_audit_helper.php
Line: 176
Function: file_get_contents

File: /var/www/html/application/helpers/my_audit_helper.php
Line: 250
Function: simplexml_load_file_from_url

File: /var/www/html/application/helpers/my_audit_helper.php
Line: 1034
Function: getPubMedXML

File: /var/www/html/application/helpers/my_audit_helper.php
Line: 3152
Function: GetPubMedArticleOutput_2016

File: /var/www/html/application/controllers/Detail.php
Line: 575
Function: pubMedSearch_Global

File: /var/www/html/application/controllers/Detail.php
Line: 489
Function: pubMedGetRelatedKeyword

File: /var/www/html/index.php
Line: 316
Function: require_once

Effect of different debonding techniques on shear bond strength and enamel cracks in simulated clinical set-ups. | LitMetric

Effect of different debonding techniques on shear bond strength and enamel cracks in simulated clinical set-ups.

J World Fed Orthod

Postgraduate Student of Orthodontics, Dental Research Center, Research Institute of Dental Sciences, Shahid Beheshti University of Medical Sciences, Tehran, Iran. Electronic address:

Published: March 2020

Objective: The aim of this study was to evaluate the relationship between debonding forces and enamel cracks length change between different debonding techniques.

Methods: 80 extracted premolar teeth with intact buccal enamel were divided into five groups. In each group, enamel cracks were evaluated by stereomicroscope before and after debonding. All teeth were bonded with metal brackets by self-cure adhesive (3M, USA) and then debonded by bracket debonding plier, fixed on the UTM machine, through five methods based on location of plier on brackets: OGwing (occlusogingival), MDwing (mesiodistal), Oblique, OGbase (occlusogingival) and Cusp-base.

Results: Based on non-parametric distribution of data, there was no significant difference between groups in ARI and enamel cracks length change. The highest shear bond strength for debonding presented in OG base method (25.25 ± 8.4) and the difference was statistically significant (P-value = 0.029). There was no linear relationship between shear bond strength and cracks length change and also between ARI and cracks length change.

Conclusion: Despite the lower cracks length change in Cusp-base method than other groups, there wasn't significant difference between debonding methods. Also the amount of debonding forces and ARI do not affect the changes of cracks length.

Download full-text PDF

Source
http://dx.doi.org/10.1016/j.ejwf.2019.11.003DOI Listing

Publication Analysis

Top Keywords

cracks length
24
enamel cracks
16
length change
16
shear bond
12
bond strength
12
debonding
8
cracks
8
debonding forces
8
length
6
enamel
5

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!