Background: The results of total hip arthroplasty (THA) with use of Delta ceramic articulation were successful at medium term follow-up. The use of this newest ceramic has markedly reduced the incidence of ceramic head fractures, but not the incidence of ceramic liner fractures. We tested a hypothesis that the ceramic fractures are prevented by use of a metal shell with 18° inner taper angle and a stem design with a reduced neck geometry.
Methods: We conducted a prospective multicenter study of cementless THA with use of 32/36-mm Delta ceramic bearing, Exceed ABT metal shell and Taperloc stem. We evaluated ceramic fracture, noise, clinical results, radiological changes and survival rate at a minimum of 5-year follow-up.
Results: From April 2010 to February 2012, 246 patients (274 THAs) were enrolled. Among them, 224 patients (130 men and 94 women, 250 hips) were followed-up for 5-8 years (mean 6.0 years). Ceramic malseating or fracture did not occur in any patient. Eight patients (8 hips, 3.2%) reported noise. Mean Harris hip score was 84 points at the latest follow-up. All acetabular and femoral components had bone-ingrown stability. Two hips were revised due to recurrent dislocation and periprosthetic fracture. The survival rate was 99.6% at 8 years postoperatively.
Conclusion: Ceramic fractures can be prevented by a use of (1) 32/36-mm Delta ceramic bearing, (2) metal shell with 18° taper angle, and (2) stem with a reduced neck geometry. However, noise remains a concern of the Delta ceramic bearing.
Level Of Evidence: Therapeutic level II.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1007/s00402-020-03515-2 | DOI Listing |
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!