Non-volatile immobilization of iodine by the cold-sintering of iodosodalite.

J Hazard Mater

Department of Nuclear and Quantum Engineering, KAIST, Daejeon 34141, Republic of Korea; Department of Materials Science and Engineering, KAIST, Daejeon, 34141, Republic of Korea. Electronic address:

Published: March 2020

A cold-sintering process at a very low temperature (300 °C) achieved stable immobilization of simulated radioiodine waste incorporated in sodalite (iodosodalite). The reported sintering temperature was much lower than conventional ceramic waste form processing temperatures (600-1100 °C) and had no effect on the stability of the loaded iodine waste. Excellent iodine retention (>93%) with relative sintered density 91% were achieved by the cold-sintering at 300 °C, respectively. The sintered body exhibited a micro-hardness value of 3.9 ± 0.1 GPa and compressive strength of 198 ± 11 MPa. The seven-day product consistency test found iodine leaching rates on order of the magnitude 10 g/m⋅d. These results are the first example of the low temperature consolidation of iodine-bearing sodalite without using any additional material (e.g. glass, cement, etc.). High retention of the loaded simulated radioiodine without volatilization warrants the cold-sintering process for the environmental-friendly disposal of radioiodine.

Download full-text PDF

Source
http://dx.doi.org/10.1016/j.jhazmat.2019.121646DOI Listing

Publication Analysis

Top Keywords

cold-sintering process
8
low temperature
8
simulated radioiodine
8
non-volatile immobilization
4
iodine
4
immobilization iodine
4
cold-sintering
4
iodine cold-sintering
4
cold-sintering iodosodalite
4
iodosodalite cold-sintering
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!