End of life photovoltaic panels of different technologies (poly crystalline Si, amorphous Si, and CdTe) were treated mechanically in pilot scale by single shaft shredder minimizing the production of fine fractions below 0.4 mm (<18% weight). Grounded material was sieved giving: an intermediate fraction (0.4-1 mm) of directly recoverable glass (18% weight); a coarse fraction (which should be further treated for encapsulant removal), and fine fractions of low-value glass (18%), which can be treated by leaching for the removal of metal impurities. Encapsulant removal from coarse fraction was successfully performed by solvent treatment using cyclohexane at 50 °C for 1 h giving high-grade glass (52% weight), which can be reused for panel production. Experimental results of solvent treatment were compared with those from thermal treatment by economic analysis and Life Cycle Assessment, denoting in both cases the advantages of solvent treatment in recovering high-value glass.

Download full-text PDF

Source
http://dx.doi.org/10.1016/j.jenvman.2019.109313DOI Listing

Publication Analysis

Top Keywords

life photovoltaic
8
photovoltaic panels
8
solvent versus
4
versus thermal
4
thermal treatment
4
treatment glass
4
glass recovery
4
recovery life
4
panels environmental
4
environmental economic
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!