It evaluated the effect of aging by Low Temperature Degradation (LTD), executed after post- processing surface treatments (polishing, heat treatment and glazing), on the surface characteristics (micromorphology and roughness) and on the structural stability (phase transformation and mechanical behavior-flexural strength and structural reliability) of a ground yttrium-stabilized tetragonal zirconia polycrystal (Y-TZP) ceramic. Discs of Y-TZP (VITA In-Ceram YZ) were manufactured (ISO:6872-2015; 15 mm in diameter and 1.2 ± 0.2 mm in thickness) and randomly assigned into 10 groups according two factors: "aging" in 2 levels (with or without) and "surface treatment" in 5 levels (Ctrl: as-sintered; Gr: grinding with coarse diamond bur; Gr + HT: grinding plus heat treatment; Gr + Pol: grinding plus polishing; Gr + Gl: grinding plus glazing). Roughness (n=30), biaxial flexural test (n=30), phase transformation (n=2), and surface topography (n=2) analyses were performed. Aging led to an intense increase in monoclinic (m) phase content for all the tested conditions, being the as-sintered samples (Ctrl= 65.6%) more susceptible to the t-m phase transformation. Despite of increasing the m-phase content, aging was not detrimental for characteristic strength (except to the grinding condition). There was no significant reduction in the Weibull modulus after surface treatments. Additionally, heat treatment and glazing after grinding led to a decrease in characteristic strength, while polishing presented the highest characteristic strength values. Thus, polishing is mandatory after grinding the Y-TZP ceramic, while performing glazing or heat-treatment alone after grinding lead to the worst mechanical performance.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1590/0103-6440201802044 | DOI Listing |
J Int Soc Prev Community Dent
October 2024
Department of Basic Dental Science, College of Dentistry, University of Mosul, Mosul, Iraq.
Aim: To evaluate the micro-shear bond strength (µ-SBS) of resin-modified glass ionomer cement and to assess the chemical and topographical changes in the zirconia fitting surface induced by acidulated phosphate fluoride (APF) gel using scanning electron microscope (SEM) analysis and Fourier transform infrared (FTIR) spectroscopy.
Materials And Methods: Thirty-two samples were prepared from two zirconia materials, UPCERA HT White and BruxZir Solid Zirconia, milled by a computer-aided design/computer-aided manufacturing system. From each zirconia sample, six plates were prepared for FTIR and SEM testing.
Clin Oral Investig
December 2024
Department of Prosthetic Dentistry, Medical Faculty, Heidelberg University, Heidelberg, Germany.
Objectives: To prospectively evaluate the wear of posterior zirconia resin-bonded fixed partial dentures (RBFPDs) with polished occlusal surfaces and their natural enamel antagonists compared to contralateral controls in an enamel-enamel contact over 5 years.
Materials And Methods: In six patients with either an inlay- or wing-retained RBFPD made of monolithic 3 mol% yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP), wear was evaluated indirectly using baseline and annual polyvinyl siloxane impressions. Resulting gypsum models were digitized and aligned by unchanged surface areas.
Dent Mater
February 2025
Department of Prosthetic Dentistry, Dental School, Ludwig-Maximilians-Universität München, Munich, Germany.
Objective: To compare the fatigue behavior and reliability of 5 pressed lithium disilicate ceramics and a 5 mol% yttria-stabilized zirconia (5Y-TZP) when 3 dynamic loading protocols were used.
Methods: Bar-shaped specimens (30 × 4 × 3 mm) were fabricated from 5 pressed lithium disilicate ceramics (AMB, CEL, INI, IPS, and LIV) and a 5Y-TZP (ZR) (N = 324). Six specimens from each material were subjected to a static 4-point fracture load test, while the remaining specimens were subjected dynamic loading by increasing the starting load (30 % of the static fracture load) in every 5000 cycles by 50 N (loading protocol 1), in every 5000 cycles by 5 % (loading protocol 2) or in every 1000 cycles by 10 N (loading protocol 3) until fracture (n = 16).
J Prosthodont
November 2024
Gerodontology and Oral Rehabilitation, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, Tokyo, Japan.
Purpose: To evaluate the impact of varying concentrations of 3 mol% yttria-stabilized tetragonal zirconia polycrystalline ceramic (3Y-TZP) nanoparticles on mechanical properties of three-dimensional (3D)-printed resins in stereolithography (SLA) technology.
Materials And Methods: A total of four groups (n = 6) of specimens were printed. Pure 3D-printed resin was used as the control group (0 wt%).
Materials (Basel)
October 2024
Department of Prosthetic Dental Sciences, College of Dentistry, Prince Sattam Bin Abdulaziz University, Alkharj 11942, Saudi Arabia.
Surface treatment of the intaglio surface of zirconia is important for bonding. However, it could affect the strength of the materials. The purpose of this study is to compare the effect of laser, etching, and air abrasion surface treatment methods to a control group on the flexural strength of three zirconia materials with two different thicknesses.
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!