High temperature creep testing at a very low load range (<10 N) on miniaturized specimens has always been a challenge due to inherent design limitation (such as significant preload) of the conventional creep testing machines. In the present study, the challenge was overcome by developing a simple and versatile horizontal creep testing machine to conduct creep tests in the loading range of ∼6-300 N in tension and in compression. The competence of the in-house-built horizontal creep machine was validated by conducting creep testing on dog-bone shaped sheet specimens of cast Mg-1Sn-1Ca (TX11) Mg-base alloy over a lower stress range of 1.6-5.9 MPa (equivalent load range of 6.4-18.1 N) at 450 °C and in the high stress range of 20-80 MPa (equivalent load range of 76-310 N) at 175 °C.

Download full-text PDF

Source
http://dx.doi.org/10.1063/1.5040841DOI Listing

Publication Analysis

Top Keywords

creep testing
8
testing low
8
simple versatile
4
versatile machine
4
machine creep
4
low loads
4
loads 6-300
4
6-300 miniaturized
4
miniaturized specimens
4
specimens application
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!