Highly luminescent thin films of zinc tungstate (ZT) have been deposited on top of conventional scintillators (Yttrium Aluminum Perovskite, Yttrium Aluminum Garnet) for electron detection in order to replace the need for a top conducting layer, such as indium tin oxide (ITO) or aluminum, which is non-scintillating and electron absorbing. Such conventional conducting layers serve the single purpose of eliminating electrical charge build-up on the scintillator. The ZT film also eliminates charging, which has been verified by measuring the Duane-Hunt limit and electron emission versus accelerating voltage. The luminescent nature of the ZT film ensures effective detection of low energy electrons from the very top surface of the structure ZT/scintillator, which we call "first-surface scintillator". The cathodoluminescence has been measured directly with a photodetector and spectrally resolved at different accelerating voltages. All results demonstrate the extended range of operation of the first-surface scintillator, while the conventional scintillators with a top ITO layer decline below 5 kV and have practically no output below 2 kV. Scintillators of different types were integrated in a detection system for backscattered electrons (BSE). The quality of the image at high accelerating voltages is comparable with the conventional scintillator and commercial BSE detector, while the image quality at 1 kV from the first-surface scintillator is superior.

Download full-text PDF

Source
http://dx.doi.org/10.1017/S1431927618015027DOI Listing

Publication Analysis

Top Keywords

first-surface scintillator
12
accelerating voltage
8
conventional scintillators
8
yttrium aluminum
8
accelerating voltages
8
scintillator low
4
accelerating
4
low accelerating
4
voltage scanning
4
electron
4

Similar Publications

Article Synopsis
  • Proton therapy has advanced from passive scattering to more precise spot scanning technologies, enhancing dose delivery and conformity.
  • The development of the Central Axis Alignment Device (CAAD) aims to ensure accurate alignment between the Dynamic Collimation System (DCS) and the proton beam's central axis by using a camera and scintillating screen for measurement.
  • The CAAD achieves high precision in determining the offset between the DCS and proton beam alignment, improving accuracy to 0.054 mm, thus eliminating reliance on less accurate x-ray sources for calibration.
View Article and Find Full Text PDF

Highly luminescent thin films of zinc tungstate (ZT) have been deposited on top of conventional scintillators (Yttrium Aluminum Perovskite, Yttrium Aluminum Garnet) for electron detection in order to replace the need for a top conducting layer, such as indium tin oxide (ITO) or aluminum, which is non-scintillating and electron absorbing. Such conventional conducting layers serve the single purpose of eliminating electrical charge build-up on the scintillator. The ZT film also eliminates charging, which has been verified by measuring the Duane-Hunt limit and electron emission versus accelerating voltage.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!