The purpose of this study was to investigate the effect of remaining dentin thickness (RDT) and long term water storage on dentin bond strength in-vitro. Twenty-seven third molars were randomly divided into 3 groups: Clearfil Bond SE ONE (SE1, Kuraray Noritake Dental, Okayama, Japan), G-Bond plus (GB, GC, Tokyo, Japan) and Clearfil Mega Bond (MB, Kuraray Noritake Dental). Bonded specimens were stored in water at 37ºC for 24 h. The teeth were then sectioned perpendicular to the adhesive interface to produce beams. RDT of each beam was measured digital calliper. Microtensile bond strength testing was carried out at a crosshead speed of 1 mm/min after 24 h and 1 year water storage. Thicker RDT produced higher bond strengths with one/two-step self-etch materials tested except for the group of 24 h MB. Nevertheless water storage time and RDT affected µTBS in all materials used.

Download full-text PDF

Source
http://dx.doi.org/10.4012/dmj.2017-140DOI Listing

Publication Analysis

Top Keywords

water storage
16
bond strength
12
remaining dentin
8
dentin thickness
8
long term
8
term water
8
storage dentin
8
dentin bond
8
kuraray noritake
8
noritake dental
8

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!