A thermoelectric copper-iodide composite from the pyrolysis of a well-defined coordination polymer.

Dalton Trans

Institute of Materials Research and Engineering, A*STAR (Agency for Science, Technology and Research), 2 Fusionopolis Way, #08-03, Innovis, Singapore 138634, Republic of Singapore.

Published: April 2018

Coordination polymer 1 was prepared from CuI and a flexible [SNS] ligand L in acetonitrile. The thermal decomposition of 1 yielded a CuI-rich thermoelectric carbon composite 2, which is relatively light, thermally stable and robust. Composite 2 possesses high Seebeck coefficients (700-950 μV K-1) from rt to 204 °C after an optimization cycle.

Download full-text PDF

Source
http://dx.doi.org/10.1039/c8dt00090eDOI Listing

Publication Analysis

Top Keywords

coordination polymer
8
thermoelectric copper-iodide
4
copper-iodide composite
4
composite pyrolysis
4
pyrolysis well-defined
4
well-defined coordination
4
polymer coordination
4
polymer prepared
4
prepared cui
4
cui flexible
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!