Tuning defects in oxides at room temperature by lithium reduction.

Nat Commun

Department of Chemistry and Collaborative Innovation Center for Nanomaterial Science and Engineering, Tsinghua University, 100084, Beijing, China.

Published: April 2018

Defects can greatly influence the properties of oxide materials; however, facile defect engineering of oxides at room temperature remains challenging. The generation of defects in oxides is difficult to control by conventional chemical reduction methods that usually require high temperatures and are time consuming. Here, we develop a facile room-temperature lithium reduction strategy to implant defects into a series of oxide nanoparticles including titanium dioxide (TiO), zinc oxide (ZnO), tin dioxide (SnO), and cerium dioxide (CeO). Our lithium reduction strategy shows advantages including all-room-temperature processing, controllability, time efficiency, versatility and scalability. As a potential application, the photocatalytic hydrogen evolution performance of defective TiO is examined. The hydrogen evolution rate increases up to 41.8 mmol g h under one solar light irradiation, which is ~3 times higher than that of the pristine nanoparticles. The strategy of tuning defect oxides used in this work may be beneficial for many other related applications.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC5882908PMC
http://dx.doi.org/10.1038/s41467-018-03765-0DOI Listing

Publication Analysis

Top Keywords

lithium reduction
12
defects oxides
8
reduction strategy
8
hydrogen evolution
8
tuning defects
4
oxides
4
oxides room temperature
4
room temperature lithium
4
reduction
4
reduction defects
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!