Time multiplexed deep reactive ion etching of germanium and silicon-A comparison of mechanisms and application to x-ray optics.

J Vac Sci Technol B Nanotechnol Microelectron

Cornell High Energy Synchrotron Source, Cornell University, Ithaca, New York 14853.

Published: January 2018

Although the mechanisms of deep reactive ion etching (DRIE) of silicon have been reported extensively, very little by comparison has been discussed concerning DRIE of germanium. By directly comparing silicon and germanium etching in a time multiplexed DRIE process, the authors extract significant differences in etch mechanisms from a design of experiment and discuss how these differences are relevant to the design and fabrication of silicon and germanium collimating channel array x-ray optics. The differences are illuminated by characteristics such as reactive ion etching (RIE)-lag, aspect ratio dependent etching, and sidewall passivation. Specifically, the authors demonstrate the more severe nature of RIE-lag in germanium, especially at aspect ratios exceeding 13:1. In addition, the differences in the profile evolution between silicon and germanium are shown to be a result of differences in sidewall passivation. There is also a correlation between the different sidewall passivation and the inherent lack of scalloping in the case of germanium DRIE.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC5754219PMC
http://dx.doi.org/10.1116/1.4991875DOI Listing

Publication Analysis

Top Keywords

reactive ion
12
ion etching
12
silicon germanium
12
sidewall passivation
12
time multiplexed
8
deep reactive
8
x-ray optics
8
germanium
7
etching
5
differences
5

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!