Objective: The effect of dentin desensitizer Systemp on the shear bond strength of composite resin to dentin using three different bonding agents, i.e., Prime & Bond NT, Xeno V, and Futurabond DC were evaluated.
Materials And Methods: Sixty recently extracted human premolars were divided into six groups of ten teeth each. The superficial dentin was etched with 37% phosphoric acid. In Groups I, II, and III, Prime & Bond NT, Xeno V, and Futurabond DC, respectively, were applied to dentin and composite placed. Following application of dentin desensitizer Systemp in Groups IV, V, and VI, Prime & Bond NT, Xeno V, and Futurabond DC, respectively, were applied to dentin and composite placed. The shear bond strength was evaluated. Data obtained were statistically analyzed using one-way analysis of variance, post hoc, and Dunnett's test.
Results: Following application of dentin desensitizer Systemp, mean shear bond strength increased when Prime & Bond NT bonding agent was used while it decreased for Xeno V and Futurabond DC bonding agents.
Conclusion: Within the limitations of this study, it was observed that following application of dentin desensitizer Systemp, mean shear bond strength may increase or decrease depending on the bonding agents used.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC5514808 | PMC |
http://dx.doi.org/10.4103/0972-0707.209069 | DOI Listing |
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!