This study aims to quantify the biomechanical properties of murine temporomandibular joint (TMJ) articular disc and condyle cartilage using AFM-nanoindentation. For skeletally mature, 3-month old mice, the surface of condyle cartilage was found to be significantly stiffer (306±84kPa, mean±95% CI) than those of the superior (85±23kPa) and inferior (45±12kPa) sides of the articular disc. On the disc surface, significant heterogeneity was also detected across multiple anatomical sites, with the posterior end being the stiffest and central region being the softest. Using SEM, this study also found that the surfaces of disc are composed of anteroposteriorly oriented collagen fibers, which are sporadically covered by thinner random fibrils. Such fibrous nature results in both an F-D indentation response, which is a typical Hertzian response for soft continuum tissue under a spherical tip, and a linear F-D response, which is typical for fibrous tissues, further signifying the high degree of tissue heterogeneity. In comparison, the surface of condyle cartilage is dominated by thinner, randomly oriented collagen fibrils, leading to Hertzian-dominated indentation responses. As the first biomechanical study of murine TMJ, this work will provide a basis for future investigations of TMJ tissue development and osteoarthritis in various murine TMJ models.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC5582691 | PMC |
http://dx.doi.org/10.1016/j.jbiomech.2017.06.031 | DOI Listing |
Proc Natl Acad Sci U S A
January 2025
Department of Orthopedic Surgery, State Key Laboratory of Complex Severe and Rare Diseases, Peking Union Medical College Hospital, Chinese Academy of Medical Sciences and Peking Union Medical College, Beijing 100730, China.
SOX9 is a crucial transcriptional regulator of cartilage development and homeostasis. Dysregulation of is associated with a wide spectrum of skeletal disorders, including campomelic dysplasia, acampomelic campomelic dysplasia, and scoliosis. Yet how variants contribute to the spectrum of axial skeletal disorders is not well understood.
View Article and Find Full Text PDFJ Cell Physiol
January 2025
Department of Spine, Wangjing Hospital of China Academy of Chinese Medical Sciences, Beijing, China.
In this study, we explored the impact of different biomechanical loadings on lumbar spine motion segments, particularly concerning intervertebral disc degeneration (IVDD). We aimed to uncover the cellular milieu and mechanisms driving ossification in the nucleus pulposus (NP) during IVDD, a process whose underlying mechanisms have remained elusive. The study involved the examination of fresh NP tissue from the L3-S1 segment of five individuals, either with IVDD or healthy.
View Article and Find Full Text PDFAnat Rec (Hoboken)
January 2025
Department of Health and Rehabilitation Sciences, Slippery Rock University, Slippery Rock, Pennsylvania, USA.
Bones of the skull are traditionally categorized as derived from either endochondral or intramembranous bone. In our previous work, we have observed the interaction of different tissue types in growth of the skull. We find the dichotomy of intramembranous and endochondral bone to be too restrictive, limiting our interpretation of sources of biological variation.
View Article and Find Full Text PDFJ Clin Orthop Trauma
February 2025
Trauma and Orthopaedics East and North Hertfordshire NHS Trust Lister Hospital, Stevenage, UK.
Background: There has been an increasing interest in elbow hemiarthroplasty to circumvent the problems with total elbow arthroplasty for comminuted distal humerus fractures in the elderly. The primary aim of the study is to assess the mid-term clinical and radiological outcomes of patients undergoing TEA and hemiarthroplasty for distal humerus fractures.
Methods: Retrospective analysis of data for patients undergoing hemiarthroplasty for distal humerus fractures (OTA- C3 Comminuted total articular fractures) was done.
Front Endocrinol (Lausanne)
January 2025
Section on Growth and Development, Eunice Kennedy Shriver National Institute of Child Health and Human Development, National Institute of Health, Bethesda, MD, United States.
Recombinant human IGF-1 is used to treat severe primary IGF-1 deficiency, but this treatment requires twice-daily injection, often does not fully correct the growth deficit, and has important off-target effects. We therefore sought to target IGF-1 to growth plate cartilage by generating fusion proteins combining IGF-1 with single-chain human antibody fragments that target matrilin-3, a cartilage matrix protein. We previously showed that this cartilage-targeting IGF-1 fusion protein (CV1574-1) promoted growth plate function in a GH-deficient (lit) mouse model.
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!