Polyetheretherketone (PEEK) is a material suitable for frameworks of fixed dental prostheses. The effect of different surface treatments on the bond strength of PEEK bonded to human dentin was evaluated. One hundred PEEK cylinders (3 mm×3 mm) were divided into five groups according to surface treatment: silica coating, sandblasting with 45 μm Al2O3 particles, etching with 98% sulfuric acid for 5, 30 and for 60 s. These cylinders were luted with resin cement onto 50 human molars. First, each tooth was embedded in epoxy resin and the buccal dentin surface was exposed. Then, two delimited dentin areas (Æ:3 mm) per tooth were etched with 35% phosphoric acid and bonded with a two-step self-priming adhesive system. After the luting procedure the specimens were stored in water (24 h/37 °C). Shear bond strength (SBS) was tested using a universal testing machine (crosshead speed 0.5 mm/min; load cell 50 kgf) and failure types were assessed. Stress data (MPa) were analyzed using the Kruskal-Wallis test. Comparison of the proportions of different failure types was performed using the Bonferroni method (p<0.05). Kruskal-Wallis demonstrated that differences among groups were not significant (p=0.187). Mean SBS were as follows: silica coating, 2.12±1.12 MPa; sandblasting, 2.37±0.86 MPa; sulfuric acid 5 s, 2.28±1.75 MPa; sulfuric acid 30 s, 1.80±0.85 MPa; sulfuric acid 60 s, 1.67±0.94 MPa. Adhesive and mixed failures were predominant in all groups. Both physical and chemical surface treatments produced adhesion between PEEK, resin cement and dentin.

Download full-text PDF

Source
http://dx.doi.org/10.1590/0103-6440201600796DOI Listing

Publication Analysis

Top Keywords

polyetheretherketone peek
8
human dentin
8
dentin surface
8
surface treatments
8
bond strength
8
failure types
8
bonding polymer
4
polymer polyetheretherketone
4
peek
4
peek human
4

Similar Publications

This study examines the biocompatibility, osteogenic potential, and effectiveness of polyether ether ketone (PEEK) composites for treating osteonecrosis, seeking to establish a theoretical basis for clinical application. A range of PEEK composite materials, including sulfonated polyether ether ketone (SPEEK), polydopamine-sulfonated polyether ether ketone (SPEEK-PDA), bone-forming peptide-poly-dopamine-sulfonated polyether ether ketone (SPEEK-PDA-BFP), and vascular endothelial growth factor-poly-dopamine-sulfonated polyether ether ketone (SPEEK-PDA-VEGF), were constructed by concentrated sulfuric acid sulfonation, polydopamine modification and grafting of bioactive factors. The experiments involved adult male New Zealand rabbits aged 24-28 weeks and weighing 2.

View Article and Find Full Text PDF

Aim: To assess hard as well as soft peri-implant tissues within cases having two lost adjacent anterior teeth treated through placing either two implants with two separate crowns or only an implant along with a crown with a cantilever, and evaluating the effect of polyetheretherketone (PEEK) restoration on cantilever design up to 18 months after functional loading.

Materials And Methods: Twenty-seven participants (15 males and 12 females; mean age, 38.6 years; range 20-50 years) with missing two adjacent anterior teeth were treated with implant system (Flotecno implant system, Italy).

View Article and Find Full Text PDF

Aim: The aim of this study was to compare the surface roughness and color stability of polyetheretherketone (PEEK) with those of conventional interim prosthetic materials like polymethylmethacrylate, bis-acrylic composite, and rubberized diurethane dimethacrylate, following immersion in solutions of varying pH value.

Materials And Methods: A total of 320 circular discs with 10 mm diameter and 2 mm height were divided based on the fabrication ( = 80)-group A: polymethylmethacrylate; group B: bis-acrylic composite; group R: rubberized diurethane; and group P: hot-pressed PEEK-and were subjected to baseline measurement of roughness ( = 40) and color ( = 40) using 3D profilometer and UV-Vis spectrophotometer, respectively. Later, 10 samples from each group were immersed in distilled water, black coffee, green tea, and Pepsi, respectively, for 120 days, and measurements of roughness and color were repeated.

View Article and Find Full Text PDF

Objective: The purpose of this study was to evaluate the effect of different preparation depths (0, 2 and 4 mm) of different restoration designs (classic endocrown design versus overlay design) on marginal adaptation of restorations fabricated of two different restorative materials (lithium disilicate and PEEK).

Materials And Methods: Sixty mandibular natural molars were collected as abutments for the restorations of this study, and grouped in three main groups of different cavity depths (0, 2 and 4). Each group was divided into two subgroups according to material of fabrication to (L) for lithium disilicate (IPS emax CAD, Ivoclar vivadent, Switzarland) and (P) for PEEK (Bio-hpp, Bredent, Germany).

View Article and Find Full Text PDF

Carbon fibre reinforced polyetheretherketone (CFR-PEEK) implants have gained interest because of reported biomechanical advantages and radio-lucent properties. The aim of this study was to evaluate the role of CFR-PEEK nails in patients with metastatic bone disease (MBD). We performed a retrospective cohort study evaluating patients with MBD undergoing intramedullary (IM) nailing for prophylaxis or fixation of pathological fractures using CFR- PEEK or titanium implants.