Objective: The aim of the present study was to analyze biofilm formation on four different titanium-based surfaces (machined titanium zirconium (TiZr) alloy, M; machined, acid-etched TiZr alloy, modMA; machined, sandblasted, acid-etched TiZr alloy, modSLA; and micro-grooved titanium aluminum vanadium alloy, TAV MG) in an experimental human model.
Material And Methods: Custom-made discs were mounted in individual intraoral splint housings and worn by 16 volunteers for 24 h. The safranin staining assay, isothermal microcalorimetry (IMC), and SEM were applied before and after surface cleaning.
Results: The hydrophilic surfaces modMA and modSLA with greater surface micro-roughness exhibited significantly more biofilm than the hydrophobic surfaces TAV MG and M. The standardized cleaning procedure substantially reduced the biofilm mass on all surfaces. After cleaning, the IMC analyses demonstrated a longer lag time of the growth curve on TAV MG compared to modSLA. Inter- and intraindividual variations in biofilm formation on the titanium discs were evident throughout the study.
Conclusions: Surface hydrophilicity and roughness enhanced biofilm formation in vivo, whereas surface topography was the most influential factor that determined surface cleanability. While the grooved surface retained larger amounts of initial biofilm, the machined surface was easier to clean, but proliferation indicated by increased metabolic activity (growth rate) in IMC occurred despite mechanical biofilm removal.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1111/clr.12821 | DOI Listing |
Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!