Background/aims: As restful, non-interrupted sleep is essential for normal mental and physical functioning, the urine flow rate (UFR) overnight remains low. Due to this reduced UFR, the kidneys produce a lower urine volume, which may lead to supersaturation of lithogens in the renal collecting system. The protective mechanisms that prevent the rise in the concentration of the lithogenic substances in urine, such as calcium phosphate, are explored.

Methods: Urine samples were collected from 26 subjects every 2-3 h during daylight with one nocturnal collection; the UFR was calculated in the median time for each collection period. Urinary constituents for calcium phosphate precipitation including electrolytes, calcium, phosphate, citrate, and pH were measured. Comparisons within individuals were done by paired t test.

Results: The calcium excretion rate fell significantly overnight (from 2.4 ± 0.2 µmol/min during the daytime to 1.5 ± 0.3 µmol/min, p < 0.05), in parallel with sodium excretion (54 ± 16 µmol/min from its daytime 127 ± 12 µmol/min, p < 0.05), preventing nocturnal calcium concentration from increasing (3.0 ± 0.3 mmol/l daytime to 2.5 ± 0.5 mmol/l overnight), while citrate concentration did not change significantly. The total urine phosphate concentration rose significantly overnight (daytime 18.7 ± 1.4 µmol/min vs. nocturnal 20.9 ± 1.7 µmol/min), but the concentration of divalent phosphate did not increase in the overnight period.

Conclusions: Although the UFR was lower overnight, there was no evidence that the risk of calcium phosphate precipitate formation in healthy subjects was increased.

Download full-text PDF

Source
http://dx.doi.org/10.1159/000443993DOI Listing

Publication Analysis

Top Keywords

calcium phosphate
24
protective mechanisms
8
calcium
8
phosphate
8
phosphate precipitation
8
µmol/min daytime
8
µmol/min 005
8
overnight
7
µmol/min
6
urine
5

Similar Publications

: The synthesis of fluoridated apatite consists of several stages, among which the heat treatment has a significant impact on the physical and chemical properties. The present study aims to elucidate the influence of two different sintering methods on fluoride-substituted apatite properties. : For this purpose, a two F-substituted apatites were produced by heat treatment in different ways called "rapid sintering" and "slow sintering".

View Article and Find Full Text PDF

Comparative Study of Anti-COVID Mouthwash and Remineralization Agents on Dentinal Tubular Occlusion: An Study.

J Int Soc Prev Community Dent

December 2024

Assistant professor, Oral and Dental Disease Research Center, Department of Operative Dentistry, Faculty of Dentistry, Zahedan University of Medical Sciences, Zahedan, Iran.

Aim: Tooth sensitivity caused by exposed dentin tubules is a common clinical problem requiring correct treatment methods. Owing to the spread of the COVID-19 virus, it has become common to use different mouthwashes, including 1.5% hydrogen peroxide (HP), before dental procedures.

View Article and Find Full Text PDF

Matrix vesicle-inspired delivery system based on nanofibrous chitosan microspheres for enhanced bone regeneration.

Mater Today Bio

February 2025

State Key Laboratory of Oral & Maxillofacial Reconstruction and Regeneration, Key Laboratory of Oral Biomedicine Ministry of Education, Hubei Key Laboratory of Stomatology, School & Hospital of Stomatology, Wuhan University, Wuhan, 430079, China.

Inspired by the initial mineralization process with bone matrix vesicles (MVs), this study innovatively developed a delivery system to mediate mineralization during bone regeneration. The system comprises nanofibrous chitosan microspheres (NCM) and poly (allylamine hydrochloride)-stabilized amorphous calcium phosphate (PAH-ACP), which is thereafter referred to as NCMP. NCM is synthesized through the thermal induction of chitosan molecular chains, serving as the carrier, while PAH-ACP functions as the mineralization precursor.

View Article and Find Full Text PDF

Background: Prosthetic joint infection is a serious complication that can arise after total joint replacement surgery. When bacteria colonise an orthopaedic implant, they form biofilms that protect them from their environment, making them difficult to remove. Treatment is further complicated by a global rise of antimicrobial resistance.

View Article and Find Full Text PDF

Following implantation, infections, inflammatory reactions, corrosion, mismatches in the elastic modulus, stress shielding and excessive wear are the most frequent reasons for orthopedic implant failure. Natural polymer-based coatings showed especially good results in achieving better cell attachment, growth and tissue-implant integration, and it was found that the inclusions of nanosized fillers in the coating structure improves biomineralization and consequently implant osseointegration, as the nanoparticles represent calcium phosphate nucleation centers and lead to the deposition of highly organized hydroxyapatite crystallites on the implant surface. In this study, magnetic nanoparticles synthesized by the co-precipitation method were used for the preparation of cellulose acetate composite coatings through the phase-inversion method.