A plasma spraying process for the deposition of three-dimensional capillary-porous titanium coatings using a wire has been developed. In this process, two additional dc arcs are discharged between plasmatron and both the wire and the substrate, resulting in additional activation of the substrate and the particles, particularly by increasing their temperature. The shear strength of the titanium coating with 46% porosity is 120.6 MPa. A new procedure for estimating the shear strength of porous coatings has been developed.

Download full-text PDF

Source
http://dx.doi.org/10.1016/j.msec.2015.11.033DOI Listing

Publication Analysis

Top Keywords

shear strength
12
three-dimensional capillary-porous
8
capillary-porous titanium
8
titanium coatings
8
strength three-dimensional
4
coatings intraosseous
4
intraosseous implants
4
implants plasma
4
plasma spraying
4
spraying process
4

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!