Nanofibers were prepared from polycaprolactone, polylactide and polyvinyl alcohol using Nanospider(TM) technology. Polyethylene glycols with molecular weights of 2 000, 6 000, 10 000 and 20 000 g/mol, which can be used to moderate the release profile of incorporated pharmacologically active compounds, served as model molecules. They were terminated by aromatic isocyanate and incorporated into the nanofibers. The release of these molecules into an aqueous environment was investigated. The influences of the molecular length and chemical composition of the nanofibers on the release rate and the amount of released polyethylene glycols were evaluated. Longer molecules released faster, as evidenced by a significantly higher amount of released molecules after 72 hours. However, the influence of the chemical composition of nanofibers was even more distinct - the highest amount of polyethylene glycol molecules released from polyvinyl alcohol nanofibers, the lowest amount from polylactide nanofibers.

Download full-text PDF

Source
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC4660903PMC
http://dx.doi.org/10.3762/bjnano.6.198DOI Listing

Publication Analysis

Top Keywords

000 000
12
model molecules
8
polyvinyl alcohol
8
polyethylene glycols
8
nanofibers release
8
chemical composition
8
composition nanofibers
8
amount released
8
molecules released
8
nanofibers
7

Similar Publications

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!