Purpose: We developed an in vitro model-blink cell that reproduces the mechanism of in vivo fouling of soft contact lenses. In the model-blink cell, model tear lipid directly contacts the lens surface after forced aqueous rupture, mirroring the pre-lens tear-film breakup during interblink.

Methods: Soft contact lenses are attached to a Teflon holder and immersed in artificial tear solution with protein, salts, and mucins. Artificial tear-lipid solution is spread over the air/tear interface as a duplex lipid layer. The aqueous tear film is periodically ruptured and reformed by withdrawing and reinjecting tear solution into the cell, mimicking the blink-rupture process. Fouled deposits appear on the lenses after cycling, and their compositions and spatial distributions are subsequently analyzed by optical microscopy, laser ablation electrospray ionization mass spectrometry, and two-photon fluorescence confocal scanning laser microscopy.

Results: Discrete deposit (white) spots with an average size of 20 to 300 μm are observed on the studied lenses, confirming what is seen in vivo and validating the in vitro model-blink cell. Targeted lipids (cholesterol) and proteins (albumin from bovine serum) are identified in the discrete surface deposits. Both lipid and protein occur simultaneously in the surface deposits and overlap with the white spots observed by optical microscopy. Additionally, lipid and protein penetrate into the bulk of tested silicone-hydrogel lenses, likely attributed to the bicontinuous microstructure of oleophilic silicone and hydrophilic polymer phases of the lens.

Conclusions: In vitro spoilation of soft contact lenses is successfully achieved by the model-blink cell confirming the tear rupture/deposition mechanism of lens fouling. The model-blink cell provides a reliable laboratory tool for screening new antifouling lens materials, surface coatings, and care solutions.

Download full-text PDF

Source
http://dx.doi.org/10.1097/OPX.0000000000000625DOI Listing

Publication Analysis

Top Keywords

model-blink cell
24
soft contact
16
contact lenses
16
vitro spoilation
8
lenses model-blink
8
vitro model-blink
8
tear solution
8
optical microscopy
8
white spots
8
surface deposits
8

Similar Publications

Novel in vitro method to determine pre-lens tear break-up time of hydrogel and silicone hydrogel contact lenses.

Cont Lens Anterior Eye

April 2019

Centre for Ocular Research & Education (CORE, formerly CCLR), School of Optometry and Vision Science, 200 University Avenue West, Waterloo, ON, N2L 3G1, Canada.

Purpose: To develop an in vitro model to determine pre-lens non-invasive break-up time (NIBUT) and to subsequently use this method to compare the NIBUT over contemporary daily disposable (DD) contact lenses (CL).

Methods: Three silicone hydrogel (SH) and two conventional hydrogel (CH) DD CLs were incubated in an artificial tear solution (ATS). A model blink cell (MBC) was utilised to mimic intermittent air exposure.

View Article and Find Full Text PDF

In Vitro Spoilation of Silicone-Hydrogel Soft Contact Lenses in a Model-Blink Cell.

Optom Vis Sci

July 2015

*PhD †MS Department of Chemical and Biomolecular Engineering, University of California, Berkeley, Berkeley, California (C-CP, NPF, CJR); Protea Biosciences Group, Morgantown, West Virginia (TR); and Vision Science Graduate Program, University of California, Berkeley, Berkeley, California (CJR).

Purpose: We developed an in vitro model-blink cell that reproduces the mechanism of in vivo fouling of soft contact lenses. In the model-blink cell, model tear lipid directly contacts the lens surface after forced aqueous rupture, mirroring the pre-lens tear-film breakup during interblink.

Methods: Soft contact lenses are attached to a Teflon holder and immersed in artificial tear solution with protein, salts, and mucins.

View Article and Find Full Text PDF

The impact of intermittent air exposure on lipid deposition.

Optom Vis Sci

November 2012

Centre for Contact Lens Research, School of Optometry and Vision Science, University of Waterloo, Waterloo, Ontario, Canada.

Purpose: To analyze the impact of intermittent air exposure on the in vitro deposition of two radioactive lipids on various contact lens (CL) materials, using a custom-designed model blink cell.

Methods: Six different CL materials (balafilcon A, lotrafilcon B, comfilcon A, senofilcon A, etafilcon A, and omafilcon A) were mounted on the model blink cell pistons, which cycled the lenses in and out of a complex artificial tear solution (ATS) that contained a trace amount of C-cholesterol or C-phosphatidylcholine. For the short-term experiment, air-exposed lenses were continuously cycled in and out of the ATS for 10 h.

View Article and Find Full Text PDF

Want AI Summaries of new PubMed Abstracts delivered to your In-box?

Enter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!