Biomedical implants made of titanium-based materials are expected to have certain essential features including high bone-to-implant contact and optimum osteointegration, which are often influenced by the surface topography and physicochemical properties of titanium surfaces. The surface structure in the nanoscale regime is presumed to alter/facilitate the protein binding, cell adhesion and proliferation, thereby reducing post-operative complications with increased lifespan of biomedical implants. The novelty of our TiO2 nanostructures lies mainly in the high level control over their morphology and roughness by mere compositional change and optimisation of the experimental parameters. The present work focuses on the wetting behaviour of various nanostructured titanium surfaces towards water. Kinetics of contact area of water droplet on macroscopically flat, nanoporous and nanotubular titanium surface topologies was monitored under similar evaporation conditions. The contact area of the water droplet on hydrophobic titanium planar surface (foil) was found to decrease during evaporation, whereas the contact area of the droplet on hydrophobic nanorough titanium surfaces practically remained unaffected until the complete evaporation. This demonstrates that the surface morphology and roughness at the nanoscale level substantially affect the titanium dioxide surface-water droplet interaction, opposing to previous observations for microscale structured surfaces. The difference in surface topographic nanofeatures of nanostructured titanium surfaces could be correlated not only with the time-dependency of the contact area, but also with time-dependency of the contact angle and electrochemical properties of these surfaces.
Download full-text PDF |
Source |
---|---|
http://dx.doi.org/10.1016/j.colsurfb.2015.03.024 | DOI Listing |
Heliyon
January 2025
University of Coimbra, CEMMPRE, ARISE, Department of Mechanical Engineering, Rua Luís Reis Santos, 3030-788, Coimbra, Portugal.
Recent advancements in aerospace industry demand intricate aero-engine parts, leading to the increased use of titanium alloys, particularly Ti-17, due to its high strength, thermal stability, and corrosion resistance. However, its low thermal conductivity and tool wear tendency pose significant machining challenges, impacting surface integrity, fatigue life, and overall component performance. This study investigates the Wire Electrical Discharge Cutting (WEDC) process, revealing that the mechanism behind improved surface integrity lies in the controlled thermal input, which minimizes phase transformations and reduces residual stresses.
View Article and Find Full Text PDFBMC Oral Health
January 2025
Department of Conservative Dentistry, School of Dentistry, Dental Research Institute, Dental and Life Science Institute, Pusan National University, Yangsan, Korea.
Background: This study compared the torsional resistance, bending stiffness, and cyclic fatigue resistances of different heat-treated NiTi files for minimally invasive instrumentation.
Methods: TruNatomy (TN) and EndoRoad (ER) file systems were compared with ProTaper Gold (PG). Torsional load, distortion angle, and bending stiffness were assessed using a custom device AEndoS, and toughness was calculated using the torsional data.
Zhonghua Kou Qiang Yi Xue Za Zhi
January 2025
Department of Stomatology, Affiliated Hospital of Putian University, Putian 351106, China.
To investigate the effect of the sizes of osteon-like concentric microgroove structures on the osteoclastic differentiation of macrophages on titanium surfaces, and to provide reference for the surface modification of implants. The silicon wafers sputtered with titanium were selected as the control group (smooth surface specimens) and four concentric groups (concentric circles with the maximum diameter of 200 μ m, the minimum diameter of 20 μ m, the spacing of concentric circles of 10 or 30 μm, the width of microgrooves of 10 or 30 μm, and the depth of microgrooves of 5 or 10 μm) specimens (the total sample size in each group was 27). The width of microgrooves of C10-5 and C10-10 groups was 10 μm, the depth was 5 and 10 μm, and the width of microgrooves of C30-5 and C30-10 groups was 30 μ m, the depth was 5 and 10 μ m, respectively.
View Article and Find Full Text PDFSmall
January 2025
Department of Microelectronics, Faculty of Electrical Engineering, Mathematics and Computer Science, Delft University of Technology, Delft, 2628 CN, The Netherlands.
Miniaturization of next-generation active neural implants requires novel micro-packaging solutions that can maintain their long-term coating performance in the body. This work presents two thin-film coatings and evaluates their biostability and in vivo performance over a 7-month animal study. To evaluate the coatings on representative surfaces, two silicon microchips with different surface microtopography are used.
View Article and Find Full Text PDFRSC Adv
January 2025
Jiangsu Key Laboratory of Marine Biological Resources and Environment, Jiangsu Ocean University Lianyungang 222005 China
A Ti-MCM-41 mesoporous molecular sieve catalyst was prepared by a hydrothermal method. Nitrogen adsorption desorption, XRD, TEM and SEM characterization results showed that the catalyst had a large specific surface area, a regular hexagonal pore structure, and titanium doping was uniformly dispersed in MCM-41 molecular sieves. The amount of titanium doping, reaction temperature, and the initial solution pH had important effects on the catalytic ozonation of dimethyl phthalate (DMP) by Ti-MCM-41.
View Article and Find Full Text PDFEnter search terms and have AI summaries delivered each week - change queries or unsubscribe any time!