Thio-urethanes were synthesized by combining 1,6-hexanediol-diissocyante (aliphatic) with pentaerythritol tetra-3-mercaptopropionate (PETMP) or 1,3-bis(1-isocyanato-1-methylethyl)benzene (aromatic) with trimethylol-tris-3-mercaptopropionate (TMP), at 1:2 isocyanate:thiol, leaving pendant thiols. Oligomers were added at 10-30 phr to BisGMA-UDMA-TEGDMA (5:3:2, BUT). 25 wt% silanated inorganic fillers were added. Commercial cement (Relyx Veneer, 3M-ESPE) was also evaluated with 10-20 phr of aromatic oligomer. Near-IR was used to follow methacrylate conversion (DC) and rate of polymerization (Rpmax). Mechanical properties were evaluated in three-point bending (ISO 4049) for flexural strength/modulus (FS/FM, and toughness), and notched specimens (ASTM Standard E399-90) for fracture toughness (KIC). Polymerization stress (PS) was measured on the Bioman. Volumetric shrinkage (VS, %) was measured with the bonded disk technique. Results were analyzed with ANOVA/Tukey's test (α=5%). In general terms, for BUT cements, conversion and mechanical properties in flexure increased for selected groups with the addition of thio-urethane oligomers. The aromatic versions resulted in greater FS/FM than aliphatic. Fracture toughness increased by two-fold in the experimental groups (from 1.17 ± 0.36 MPam(1/2) to around 3.23 ± 0.22 MPam(1/2)). Rpmax decreased with the addition of thio-urethanes, though the vitrification point was not statistically different from the control. VS and PS decreased with both oligomers. For the commercial cement, 20 phr of oligomer increased DC, vitrification, reduced Rpmax and also significantly increased KIC, and reduced PS and FM. Thio-urethane oligomers were shown to favorably modify conventional dimethacrylate networks. Significant reductions in polymerization stress were achieved at the same time conversion and fracture toughness increased.
Download full-text PDF |
Source |
---|---|
http://www.ncbi.nlm.nih.gov/pmc/articles/PMC4907769 | PMC |
http://dx.doi.org/10.1016/j.dental.2015.02.008 | DOI Listing |
Objectives: Thio-urethane oligomeric additives have been shown to improve the mechanical properties of dental composites and resin cements. To try to harness those same properties in dental adhesives, in this study, these oligomers (TU) were added to the matrix and/or as filler functionalization of experimental adhesives, and the effects on conversion and mechanical properties were analyzed.
Methods: BisGMA and HEMA (60/40 wt%) were used as the monomer matrix, made polymerizable by the addition of 0.
Objective: The aim of this in vitro study was to test the effect of different composite modulation protocols (pre-heating, light-curing time and oligomer addition) for bulk filling techniques on resin polymerization stress, intra-pulpal temperature change and degree of conversion.
Methods: Class I cavities (4mm depth×5mm diameter) were prepared in 48 extracted third molars and divided in 6 groups. Restorations were completed with a single increment, according to the following groups: (1) Filtek Z250XT (room temperature - activated for 20s); (2) Filtek Z250XT (at room temperature - activated for 40s); (3) Filtek Z250XT (pre-heated at 68°C - activated for 20s); (4) Filtek Z250XT (pre-heated at 68°C - activated for 40s); (5) Filtek BulkFill (at room temperature - activated for 20s); (6) Filtek Z250XT (modified by the addition of a thio-urethane oligomer at room temperature - activated for 40s).
Biomater Investig Dent
November 2019
School of Dentistry, Biomaterials and Biomechanics, Oregon Health and Science University, Portland, Oregon.
Thio-urethane oligomers improve conversion and mechanical properties of resin cements. The objective of this study was to evaluate the effect of resin cements formulated with thio-urethane (TU) oligomers on microtensile bond strength (µTBS) of ceramics to composites subjected to thermal/mechanical cycling. BisGMA/UDMA/TEGDMA (50/30/20 wt%) containg 0 (control, EC) or 20 wt% aliphatic or aromatic thiourethane (HDDI and BDI, respectively) were mixed with CQ/amine (0.
View Article and Find Full Text PDFJ Esthet Restor Dent
March 2019
Department of Biomaterials and Biomechanics, Oregon Health & Science University, Portland, Oregon.
Objective: The aim of this study was to evaluate the color parameters and optical properties of resin cements (RCs) formulated with thio-urethanes (TUs).
Materials And Methods: Six TUs were synthesized by combining thiols (pentaerythritol tetra-3-mercaptopropionate [PETMP] or trimethylol-tris-3-mercaptopropionate [TMP]) with di-functional isocyanates (1,6-Hexanediol-diissocyante [HDDI] [aliphatic-AL] or 1,3-bis(1-isocyanato-1-methylethyl) benzene [BDI] [aromatic-AR] or Dicyclohexylmethane 4,4'-Diisocyanate [HMDI] [cyclic-CC]). TUs (20 wt%) were added to a BisGMA/UDMA/TEGDMA matrix.
J Dent
June 2018
Department of Biomaterials and Oral Biology, University of São Paulo -USP, São Paulo, Brazil.
Objectives: The use of thio-urethane oligomers has been shown to significantly improve the mechanical properties of resin cements (RCs). The aim of this study was to use thio-urethane-modified RC to potentially reinforce the porcelain-RC structure and to improve the bond strength to zirconia and lithium disilicate.
Methods: Six oligomers were synthesized by combining thiols - pentaerythritol tetra-3-mercaptopropionate (PETMP, P) or trimethylol-tris-3-mercaptopropionate (TMP, T) - with di-functional isocyanates - 1,6-Hexanediol-diissocyante (HDDI) (aliphatic, AL) or 1,3-bis(1-isocyanato-1-methylethyl)benzene (BDI) (aromatic, AR) or Dicyclohexylmethane 4,4'-Diisocyanate (HMDI) (cyclic, CC).